Optically Clear Materials
Casting and Potting can be used to encapsulate sensitive electronics as well as opto-electronic devices. In the case of LEDs they can be both cast or potted.
In the casting process, liquid resin is poured into the LED chamber and cured into the shape of the cavity. This produces a stand-alone device which can then become a component in another printed circuit board assembly.
In the potting process, LEDs are already wired and connected to a circuit board or substrate. The circuit board or substrate usually already has a frame or cavity which is then filled with a liquid resin and then cured. This results in a group of LEDs set in a ready-to-go circuit board or substrate.
KRAYDEN offers a range of Encapsulants, Potting Materials and Casting Materials
KRAYDEN OPTOLINQ™ OLS-Series are a family of optically clear (often called “water-white”) liquid encapsulants that are used to encapsulate optical or optoelectronic devices that require both a high level of light transmittance as well as a good level of mechanical protection. Products in this OLS-Series family can be epoxies, silicones or hybrid technologies. They are used extensively for the encapsulation of LED devices but could be well suited for other applications that require a clear, optical grade encapsulation system.

Liquid Resins For Potting
There are three main types of liquid resin for potting and casting applications: Epoxy, Polyurethane, and Silicone.
Resin encapsulants are used to protect and insulate electronic components from harsh environments, including moisture, thermal shock, physical vibration and shock, chemicals and dust, etc, which help electronics achieve stable performance in long term. Potting resin encapsulants are widely applied due to their usage flexibility and easy automation.
In order to meet different application needs, the properties of resin encapsulants could be adjusted. There are mainly three types of resin chemistry systems being widely applied as liquid encapsulants. The comparison between the key performance considerations is shown in the table below. Some other considerations are not mentioned here, such as flame retardancy, volatility, dielectric resistance, etc.
| PROPERTIES / RESIN TYPES |
EPOXY |
POLYURETHANE |
SILICONE |
| Glass Transition Temperature |
High |
Medium/Low |
Very Low |
| Hardness (Shore) |
High Shore D |
Shore A to Shore D |
Low Shore A |
| Heat Resistance |
Tj Up To 160 ~ 180 °C |
Tj Up To 135 °C |
Tj Up To 230 ~ 260 °C |
| Flexibility |
Brittle |
Flexible, Crack Resist |
Very Flexible |
| Mechanical Strength |
High |
Medium |
Very Low |
| Chemical Resistance |
Excellent |
Good |
Poor |
| Adhesion |
Excellent |
Good |
Poor |
| Material Cost |
Medium |
Low |
High |
| Reworkability |
Very Hard |
Hard |
Easy |
| Stress & Heat During Curing |
High |
Medium |
Very Low |
| Suitable For |
- High rigid casting
- Against harsh humidty/chemical environment
- Not suitable for sensitive parts
|
- Stress-sensitive parts
- PCB with surface mount components
- Water resistant for marine application
- Flexible from soft gel to semi-rigid casting
|
- Fragile electronic components/module
- PCB with surface mount components
|
*Reworkability: Epoxy and urethane are hard materials, providing good mechanical strength and protection for electronics. Besides, their strong adhesion to components makes them very hard to remove and rework.
*Stress & Heat During Curing: Epoxy and urethane materials produce heat while curing and create stress from shrinkage. Both the heat and stress generated could cause damage to sensitive components and wire connections.
Liquid Potting Resins Key Considerations
After deciding the basic chemistry of potting materials for your applications, there are some other features to be considered while selecting.
Hardness It is a key consideration for selecting materials. Depending on your applications and purpose of encapsulating, you need different levels of hardness. Hard materials provide better mechanical protection against the environment. Soft materials absorb vibrations well and make the component easy to repair and rework.
Thermal Conductivity The components being encapsulated may generate different levels of heat in the area, especially high power electronics. Potting materials could help to dissipate heat to ensure long-term reliability of electronics. The thermal conductive value could be adjusted by adding various fillers.
Color & Viscosity Depending on the visibility requirement of your application, you may need transparent, dark opaque, or even specific colors; Generally speaking, potting materials are designed to have low viscosity (<10 Pa.s) to ensure flowability and self-leveling for easy usage. Medium and high viscosity (>100 Pa.s) products are suitable for sealing and adhesion.
Curing Process Besides the above-mentioned properties, you may consider the curing conditions like temperature and time which suit your production and also the components. Pot life and application process also.

Potting Material Application Questions
- What kind of device/component will be potted? What is the volume of the cavity or pot being filled?
- What will the operating environment be like? Temperature range?
- Will there be exposure to moisture? Solvents or other chemicals? Vibration?
- What is the acceptable curing time or gel time? What is the curing mechanism? UV? Room temperature? Oven?
- What is the coefficient of thermal expansion (CTE) of the potting compound?
- Will the material need to be flame-retardant?
- What is the desired hardness of the cured compound?
Polyurethane Resins
Polyurethane resins are the kings of process adaptability. Almost every single characteristic of the final cured resin can be dialed in and regulated by adding a little more or a little of a certain additive. Hardness, cure speed, color, gel time, viscosity, all of these can be easily adjusted to suit production requirements. Polyurethanes cure faster and at lower temperatures than epoxy. Polyurethanes have a low elastic modulus in their cured state they are better for extra delicate components such as sensors and reed switches. However, they are notorious for high moisture absorption unless a Polybutadiene base is used.
Epoxy Resins
Epoxy resin is super adhesive: making seamless uniform bonds to a wide variety of substrates and cures to become hard with high elastic modulus, great mechanical strength, and toughness. It also has absolutely unparalleled high-temperature resistance, chemical resistance, and electrical insulation. Epoxy resin cures relatively slowly especially in smaller volumes, and so may require fast-cure hardeners that generate an exothermic reaction that may damage sensitive electrical components via mechanical stress on both the components and circuit.

Silicone Resins
Silicone resins have the lowest elastic modulus when cured of all liquid resins. They have great high-temperature and chemical resistance too. Silicone resins also cure with almost no exothermic heat making them great for encapsulating highly heat sensitive components. Silicone resins are great for insulating and covering larger areas than the other two resins, however, because their base chemistry is more expensive to produce they tend to be overall more expensive than the other two. The LED share of the lighting market is set to shift from 20% to 70% by 2020, which means the overcoming years LED encapsulation will be one of the fastest growing markets for liquid encapsulation. Liquid casting and encapsulation, in general, is more adaptive with high flexibility and low throughput which matches the market trends of more diverse low quantity orders rather than long-term high quantity orders. Liquid Epoxy resin used to the king of potting and encapsulation, however, epoxy seems to be running out of room for further developments and the most exciting developments in liquid resins seem to be in polyurethane resins. This is also because polyurethanes can be so easily adapted and so better suits the current economy of diverse smaller quantity orders.
Presentations
2026 Clear Liquid Encapsulants
This presentation provides an overview of clear liquid encapsulants used to protect electronic and optoelectronic components while maintaining exceptional optical clarity. It explores material properties, curing technologies, performance requirements, and application considerations for LEDs, sensors, displays, and other devices where long-term transparency, environmental protection, and reliability are critical.
2026 Silicones for LED Encapsulation
This presentation introduces silicone encapsulation materials designed for LED packaging and high-performance lighting applications. It covers the advantages of silicone chemistry, including optical stability, thermal resistance, UV durability, and moisture protection, while reviewing material selection considerations and product solutions for enhancing LED efficiency, reliability, and service life.
Related Blogs
Yellowing in Liquid Encapsulants
James Baduria, February 2025
This blog discusses the mchanism behind yellowing in liquid encapsulants and the mitigation strategies that can be implemented to prevent it.
Understanding Gelation and Cure Behavior
James Baduria, October 2025
This blog explores the difference between premature curing and the intended chemical reactivity of epoxy formulations.
Conductive Adhesives for Camera Modules
George Kountardas, July 2025
This blog talks about the features required for electrically conductive adhesives for camera module assembly applications.