OPTOLINQ LE-2161 | Two part epoxy resin

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

OPTOLINQ LE-2161 | Two part epoxy resin

Main features

  • Low viscosity
  • Fast curing
  • High transparency and good electrical properties

Product Description

OPTOLINQ LE-2161 is a transparent, two-part epoxy resin ideal for potting small components and sealing large dot matrix panels. It offers a fast curing rate, moderate curing temperature, and low viscosity post-mixing, and delivers exceptional electrical properties and transparency upon curing. To meet specific color requirements, it can easily be colored and diffused using specialized dye concentrates and diffusant concentrates.

OPTOLINQ LE-2161 serves as an ideal option for various electronic applications, including smart rings, due to its ability to encapsulate delicate electronic components while maintaining transparency and providing robust electrical insulation.

Cure Schedule

  • 24h @ 25°C
  • 4h @ 50–60°C
Product Family

OPTOLINQ LE-2161

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Mix RatioMix Ratio
3:1
Pot LifePot Life
1.67–2 hours
Electrical Properties
Dielectric StrengthDielectric Strength
20 kV/mm
Surface ResistivitySurface Resistivity
>1.5×10¹⁵ Ohms/sq
Volume ResistivityVolume Resistivity
>1.6×10¹⁵ Ohms⋅cm
Chemical Properties
Water AbsorptionWater Absorption
0.3 %
Physical Properties
ViscosityViscosity
548 mPa.s

Additional Information

Anti-yellowing Performance of LE-2161

The following optical images of cured Optolinq LE-2161 samples (10 and 30 g) demonstrate its anti-yellowing capability under two distinct conditions: exposure to 70 °C for 18 hours and  to 85 °C, 85% RH for 24 hours. The observed cloudiness is due to the presence of an anti-yellowing filler, a critical component for smart ring technology. This filler serves a crucial purpose without compromising the transmittance of the encapsulant, although it's important to note that the material's thickness can influence this aspect.

Anti-yellowing LE-2161

 

Recommended Curing Conditions

Cure at 25 °C for 24 h or at 50–60° C for 4 h.

These guidelines offer recommended curing parameters. Define the exact curing parameters to align with your product specifications.

Precautions for Use

  1. The usable time after A and B are mixed strongly depends on the temperature and mixing volume. Higher temperatures and larger mixing volumes lead to shorter working times. Therefore, the mixing temperature and amount should be determined based on on-site procedures.
  2. Use the product in a clean and well-ventilated workplace.
  3. Wear appropriate safety equipment before use and avoid direct contact with the body. Please read the Material Safety Data Sheet (SDS) carefully before using.

Please note that the provided information is based on available data and typical conditions. For specific applications and detailed test results, refer to the actual test data and conduct appropriate certifications.

Storage and Handling

Store in a ventilated, dry, and clean environment. Keep away from fire and heat sources. It is strictly forbidden to store in outdoor environments. The validity time will vary depending on storage conditions. At proper storage conditions, Part A and Part B have a shelf life of 183 and 93 days, respectively. Shelf life can be extended by using cold storage.

 

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers