LOCTITE STYCAST PC18M
Harmonization Code : 3909.50 | Amino-resins, phenolic resins and polyurethanes, in primary forms

Main features
- Conformal Coating
- For environmental and moisture protection
- Room temperature cure
Product Description
LOCTITE STYCAST PC 18M is a solvent-based one-component urethane coating that may be cured at room temperature. This material retains its light color after long exposure to elements and provides environmental and moisture protection.
LOCTITE STYCAST PC 18M is a reworkable, solvent-resistant coating that is fluorescent under UV light. It displays no cracking and exhibits superior toughness and abrasion resistance. It is typically used as a PCB conformal coating and can operate continuously up to 110°C.
Advantages of Loctite Stycast PC 18M
- Reworkable
- Solvent resistant
- Room temperature cure
- superior toughness and abrasion resistance
- resistant to discoloration
Cure Schedule
- 2 hours @ 60°C , in an oven
Boards must be air-dried 30 to 45 minutes before curing