Coating Powders, Paints & Varnishes

Functional and decorative thermoplastic and thermoset plastic coating powders

Coatings, powders & Resins

Coating powders, and liquid resins for casting potting and encapsulation are a category of coating materials designed to encapsulate the part. The purpose of the coating or encapsulation can be decorative, in the case of different colors, but it can also be functional in that it also provides electrical insulation or mechanical protection. Powders, varnishes, and paints are all encapsulation methods that speak more about the application method than the chemistry type.

Coating powders can be broadly defined into two broad chemistry types: thermoplastics and thermoset plastics. Each type has its pros and cons and can be further subdivided into different chemistry types and then finally defined by the end-application and desired final properties.

Please continue to our Learn More section to learn more about the kinds of coating, paint and varnish types, their application methods and to understand how KRAYDEN can help you to select and order the proper coating powder, paint or varnish that is right for your application.

Frequently asked questions

Frequently Asked Questions about Coating Powders

What are the main types of coating powder?

Coating powders can be broadly divided into thermoplastics which include polyethylene (PE) and PVC and thermoset plastics which include polyester and epoxy coating powders. Both have their pros and cons.

How can coating powders be applied?

There are two basic application methods: electrostatic and hot dipping. Electrostatic application involves coating the part first and then heating it in place. Hot dipping means heating the part ahead of time and then applying the coating powder.


Learn more

Epoxy Coating Powders for Busbar Coating, Switchgear Equipment and High Voltage Fuses


For many years KRAYDEN has supplied a range of epoxy coating powders developed for medium voltage (600V – 38,000V) bus bar and switch gear applications. KRAYDEN is one of the few epoxy coating powder manufacturers with "switch panel-rated" material, meaning that their epoxy coating powders are qualified for use in Power Distribution Switch Boards. Given the critical nature of the application, the time and costs involved to pass UL-certification, major Power Management Companies reply on KRAYDEN and their family of UL-listed epoxy coating powders. All the products offered by KRAYDEN for busbar applications are UL-listed.
 Epoxy Coating Powder for Busbars
Epoxy Coating Powder for Slot Insulation of Motor Armature

Epoxy Coating Powders for Slot Insulation of Motor Iron Armatures and Stators

KRAYDEN supplies a range of epoxy coating powders developed for motor iron armatures. From incredible bed life epoxy powders to high productivity coating powders to Class H-rated coating powders, KRAYDEN has an epoxy coating powder to meet every type of motor armature insulation application. All the products offered by KRAYDEN for motor iron armature applications are UL-listed.

Epoxy Coating Powders for Resistors, Capacitors, Varistors and Passive Electronics

KRAYDEN supplies a range of epoxy coating powders developed for electrical insulation of passive electronic devices including resistors, varistors and capacitors. From incredible thermal cycle materials for Class 1 rated Ceramic Capacitors, to low cost epoxy coating powders for film wrap capacitors, KRAYDEN products pioneered this industry and continue to push the envelope for the best performing materials on the market today. Most of the products offered by KRAYDEN for passive electronics have a UL-listing.

Epoxy Coating Powder for Capacitors, Varistors, Resistors
Epoxy Coating Powder for Toroids, Magnetic and Powder Cores

Epoxy Coating Powders for Toroids, Magnetic and Powder Cores

KRAYDEN supplies a range of epoxy coating powders developed for toroids, magnetic cores and powder cores. These products are low shrinkage and low moisture absorption coating powders which maintains the stability and inductance values of the toroid cores. These products are suitable for Molypermalloy (MPP), Iron, Sendust and other alloy powder cores. Most of the products offered by KRAYDEN for powder cores have a UL-listing.

Epoxy Coating Powders as Epoxy Binder Resin for Pot Cores

KRAYDEN supplies epoxy coating powders developed specifically to act as an epoxy binder resin for pot cores used in inductor motors. These products have excellent green strength to allow the transport from the press to the oven. Once cured, these pot cores can be used at temperatures up to 180°C and maintain their mechanical properties as well as their magnetic properties.

Epoxy Binder Resin for Pot Cores

Methods of Applying Coating Powders

Electrostatic Spray Coating Powder

Electrostatic Spraying of Epoxy Coating Powder

Coating powders can be applied using an electrostatic gun. In these cases, the powder is positively charged and the part being coated in negatively charged. This allows a thin, uniform coating to be applied to the part.

The advantage of this approach is that the powder can be wiped off and reapplied if the coating is not correct, or if the masking was done incorrectly. Since the coating powder is only attached by a static charge, it can easily be wiped off. Furthermore, the thickness of the coating can be quite uniform and can be increased or decreased based on the charge applied.

Once the part is electrostatically coated, it is moved to an oven, where the coating powder is cured in place, leaving a smooth, uniform coating over the part.

Electrostatic Fluidized Bed Application of Coating Powder

Applying the coating powder using an electrostatic fluidized better is a very practical way to apply a uniform powder coating on motor iron armatures.

Similar to the electrostatic spray application, the part and powder are charged, and the powder is applied by forwarding the parts on a rotating screw over the fluidized bed. The powder adheres to the motor armature by static electricity. As the parts roll past the fluidized bed, a brush is applied to the outside of the motor iron, removing the coating powder from the outside of the motor iron where it is nopt wanted.

Once the coating powder has been removed, the parts are rolled over an induction cure copper element where the motor armatures are exposed to temperatures of up to 240°C for a few seconds to fix and cure the coating powder in place.

Electrostatic Fluidized Bed for Motor Armature Insulation with Coating Powder
 

Coating Powder for Motor Iron Armature Insulation

KRAYDEN offers a range of coating powders for slot insulation including blue, black and green variants and Class H candidates.

Coating Powder for Motor Iron Armatures Slot Insulation Blue Black Green

Technical Papers & Brochures

KRAYDEN offers a wealth of Technical Papers, Marketing Brochures, Technical Data Sheets and SDS covering our coating powders, paints and varnishes.


Read our Blog on Coating Powders

We try to post as much information as we can on our blogs, to help you find more relevant information about how to select, use and apply coating powders, varnishes and paints.


Coating Powders for Busbar Insulation

KRAYDEN offers a range of epoxy coating powders for busbar and power distribution insulation.

Coating Powder Busbar Insulation Beige

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers