HUMISEAL 802
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- UV40 Viscosity Adjustment
- 2.78 Relative Evaporation Rate
- 24-Month Shelf Life
Product Description
HumiSeal® Thinner 802 is a proprietary solvent and diluent blend formulated for use with HumiSeal® UV40 conformal coating. It is used to lower the coating’s as-supplied viscosity or restore its original viscosity during processing while maintaining the balance of the compatible coating system. The clear liquid has a relative evaporation rate of 2.78, based on butyl acetate equal to 1, and a specific gravity of 0.86.
Key features
- UV40 compatibility: Specifically identified for use with HumiSeal® UV40 conformal coating.
- Viscosity adjustment: Supports lowering the coating’s as-supplied viscosity or restoring viscosity during processing.
- Balanced solvent blend: Formulated to maintain the original system balance when added to the compatible coating.
- Clear liquid: Supplied with a specific gravity of 0.86 and a relative evaporation rate of 2.78.
Applications / Suitable for
- Adjusting the viscosity of HumiSeal® UV40 conformal coating
- Restoring the original coating viscosity during processing
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Color
clear The color
Specific Gravity
0.86 Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume.
For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
Vapor Density
4 Vapor Pressure
34 mmHg Thermal Properties
Boiling Point
98 °C The amount of degree’s needed to reach in order to make the substance boil.
Physical Properties
VOC
none Additional Information
Technical properties
As-supplied / before-processing properties
Typical as-supplied properties. Values are not intended for use as specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product type | Proprietary solvent and diluent blend | — | As supplied |
| Compatible coating | HumiSeal® UV40 | — | Manufacturer-identified compatibility |
| Color | Clear | — | As supplied |
| Average weight per gallon | 7.17 | lb/gal | At 20°C |
| Specific gravity | 0.86 | — | Typical value |
| Relative evaporation rate | 2.78 | — | Butyl acetate = 1 |
| Boiling point | 208 | °F | Typical value |
| Vapor pressure | 34 | mmHg | At 68°F |
| Vapor density | 4.0 | — | Air = 1 |
| VOC | None | g/L | Reported in the supplied TDS |
| Shelf life | 24 | months | From date of shipment |