HumiSeal 1B31EPA Acrylic Conformal Coating
Harmonization Code : 3906909090 | Acrylic polymers in primary form Others>Others
Main features
- Fast drying
- MIL‑I‑46058C qualified
- IPC‑CC‑830 compliant
Product Description
HumiSeal 1B31EPA is a fast‑drying, single‑component acrylic conformal coating designed to provide excellent moisture and environmental protection for printed circuit assemblies. The cured film exhibits outstanding flexibility, fluoresces under UV light for easy inspection, and allows straightforward repair. HumiSeal 1B31EPA is MIL‑I‑46058C qualified, IPC‑CC‑830 compliant, RoHS Directive 2002/95/EC compliant, and EPA 33/50 compliant.
Product Key Features
- Single‑component acrylic formulation
- Fast drying, enabling efficient throughput
- MIL‑I‑46058C qualified
- IPC‑CC‑830 compliant
- RoHS compliant (Directive 2002/95/EC)
- EPA 33/50 compliant
Applications
- Protection of printed circuit boards (PCBs) across industrial, automotive, aerospace, and consumer electronics
Packaging
Please select Package Size.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Density (g)
0.95 g/cm3 Film Thickness
25 - 75 µm Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
Solids
28 % Physical Properties
Viscosity
325 mPa.s Viscosity is a measurement of a fluid’s resistance to flow.
Viscosity is commonly measured in centiPoise (cP). One cP is defined as
the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP.
A product like honey would have a much higher viscosity -around 10,000 cPs-
compared to water. As a result, honey would flow much slower out of a tipped glass than
water would.
The viscosity of a material can be decreased with an increase in temperature in
order to better suit an application
Thermal Properties
Glass Transition Temperature (Tg)
14 °C The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding.
The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
Operating Temperature
-65 - 125 °C Electrical Properties
Breakdown Voltage
6300 V Breakdown voltage is the minimum voltage necessary to force an insulator to conduct some amount of electricity.
It is the point at which a material ceases to be an insulator and becomes a resistor that conducts electricity at some proportion of the total current.
After dielectric breakdown, the material may or may not behave as an insulator any more because of the molecular structure alteration. The current flow tend to create a localised puncture that totally alters the dielectric properties of the material.