LOCTITE ECCOBOND 3707

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 3217

Main features

  • UV & Heat cure
  • One component
  • BGA cornerbond

Product Description

LOCTITE ECCOBOND 3707 UV curable edgebond is designed for bonding various types of electronic components on a PCB. It mainly plays a structural role in the packaging process.

LOCTITE ECCOBOND 3707 is a white, single component epoxy that is typically used for UV Curable CSP (Chip Scale Packages) and as a BGA (Ball Grid Array) Cornerbond.

UV Cure:

  • >3,000mJ or
  • >30 seconds @ 100 mW/cm²

Minimum intensity of 100 mW/cm² is recommended for the UV lamp

Oven Cure:

  • 2 minutes @ 130°C
Product Family

ECCOBOND 3707

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 43 days
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot LifePot Life
168 hours
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
53 °C
Physical Properties
ViscosityViscosity
9,595 mPa.s

Additional Information

UV/Light Cure Strengths

  • One component
  • No solvents
  • Very fast room temperature cure
  • Cure on demand-facilitates parts alignment
  • Less equipment space and energy
  • Fast through put-low WIP

 

UV/Light Cure Limitations

  • Sensitive to light-requires special space lighting
  • Oxygen inhibits cure
  • Line of sight cure- shadowed areas require secondary cure
  • High CTE- fillers used to lower CTE block UV/light

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers