DOWSIL RSN-0806
Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other
Main features
- Colored Baking-Enamel Resin
- Up to 538 deg C Temperature Use
- Standalone or Blendable Resin Use
Product Description
DOWSIL™ RSN-0806 Resin is a silanol-functional silicone binder resin supplied as a 50% solids, solvent-borne solution for high-temperature coating formulations. It is designed primarily for colored baking enamels used on space heaters, stoves, and similar equipment. The resin provides stability and high-temperature performance and may be used alone or blended with DOWSIL™ RSN-0805 Resin to enhance coating flexibility.
Key features
- High-temperature coating binder: Supports coating formulations intended for service at temperatures up to 538°C (1000°F).
- Silanol-functional resin: Provides a reactive silicone binder for heat-cured coating systems.
- Formulation versatility: Can be used alone or blended with DOWSIL™ RSN-0805 Resin to enhance film flexibility.
- Pre-catalyzed formulation: Supplied with catalyst to support heat-curing applications.
Applications / Suitable for
- Colored baking enamels
- High-temperature coatings for space heaters
- High-temperature coatings for stoves and similar equipment
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Specific Gravity
1.02 Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume.
For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
Physical Properties
Viscosity
150 mPa.s Viscosity is a measurement of a fluid’s resistance to flow.
Viscosity is commonly measured in centiPoise (cP). One cP is defined as
the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP.
A product like honey would have a much higher viscosity -around 10,000 cPs-
compared to water. As a result, honey would flow much slower out of a tipped glass than
water would.
The viscosity of a material can be decreased with an increase in temperature in
order to better suit an application
Thermal Properties
Flash Point
45 °C The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor.
Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
Additional Information
Technical properties
As-supplied / before-processing properties
Typical as-supplied properties. Values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Composition | Silanol-functional silicone resin in solvent | — | As supplied; pre-catalyzed |
| Diluent | Toluene/xylene | — | As supplied |
| Resin solids | 50 | % by weight | 0.5 g, 1 hour at 110°C (230°F) |
| Resin solids by volume | 41 | % | Typical value |
| Dynamic viscosity | 150 | cP | Typical value |
| Specific gravity | 1.02 | — | At 25°C (77°F) |
| Volatile organic content | 515 (4.3) | g/L (lb/gal) | EPA Reference Method 24 |
| Flash point, closed cup | 7 (45) | °C (°F) | Closed cup |
| Theoretical silicon dioxide content | 52 | % | By weight |
| Phenyl/methyl ratio | 1.2/1.0 | — | Typical value |
| Degree of substitution | 1.4 | — | Organic groups attached per silicon atom |
| Shelf life | 1080 | days | From date of manufacture when stored in the original unopened container |