DMI-3850 | Low Outgassing Adhesive
Harmonization Code : 3707.90.90.00 | Chemical preparations for photographic uses (other than varnishes, glues, adhesives and similar preparations); unmixed products for photographic uses, put up in measured portions or put up for retail sale in a form ready for use : Other : Other
Main features
- UV Cure
- Space applications
- Virtually no outgassing
Product Description
DMI-3850 is a proprietary, UV-curable adhesive specially designed for space applications with a need for low/no VOC content and virtually no outgassing. DMI-3850 contains no photoinitiators or polymerization inhibitors that can contribute to weight loss issues. In its cured state DMI-3850 is a soft and rubber-like solid and is suitable for a number of applications as a cushioning/adhesive material for space applications. The material is solvent-free, very high flash point and not DG for transport.
DMI-3850 is recommended for use as an adhesive in applications demanding low VOC and outgassing (e.g. space). DMI-3850 is self-reactive and does not require the use of a photoinitiator for UV curing. The amount of UV energy required to fully cure the material must be determined by the customer. Since the curing rate of DMI-3850 is slower than typical photoinitiator-cured materials it is suggested that curing take place in an air inhibited environment (e.g. inert gas atmosphere, between glass plates, etc.)
Packaging
Please select Package Type.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Appearance
Clear Appearance at room temperature.