DK15-0907 | Red Insulating Epoxy Coating Powder
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other






Main features
- DK15-0907 Coating Powder
- Red, insulating, epoxy based
- For low and medium voltage bus bars
Product Description
DK15-0907 Red is an epoxy-based, "One Powder Solution" coating powder developed for low and medium voltage (600V - 38,000V) bus bars. Used for over 20 years by major power distribution companies for low and medium-voltage bus bar applications, DK15-0907 provides a smooth surface appearance with high edge coverage. The fusion bonded coating is smooth, tough, and moisture-resistant for applications up to 38 KV. DK15-0907 is UL recognized for UL94-V0 rating and meets the UL746B Relative Thermal Index (RTI) of 130°C and is currently on test for an RTI at or above 150°C. Rapid and thick build reduces production cycle times. Particle size is optimized for the fluidized bed coating process.
Advantages of DK15-0907 for Busbar Coating
- Suitable for copper and aluminum bar
- Smooth, uniform coating build in excess of 200 mils (5 mm)
- Rapid build rates to reduce cycle times
- Fine grind powder to replenish size distribution
- Fluidizing agent to promote uniform build
- Ongoing testing to optimize quality & productivity
Typical applications and uses of DK15-0907 include:
- Low Voltage (600V) Copper, Aluminum and Brass Busbars
- Medium Voltage (up to 38kV) Copper, Aluminum and Brass Busbars
- Switchgear Equipment for Power Distribution
This product is no longer available. Some alternatives for busbar coating powders are:
TDS, SDS & Technical Documents
Technical Specifications
No specifications available.