BOSTIK L4045
Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

Main features
- Fast-Drying One-Part Nitrile Adhesive
- Non-Staining Bonding Formulation
- Flexible Cured Adhesive
Product Description
Bostik LIQ. 4045 is a fast-drying, one-part solvent-based nitrile adhesive formulated for bonding flexible PVC to a wide variety of substrates used in plastic upholstery and industrial assembly. The high-viscosity formulation develops high initial bond strength while producing a clear, flexible, non-staining bond line with excellent green strength. LIQ. 4045 also provides resistance to solvents and plasticizer migration, making it suitable for bonding vinyl, PVC foam, fabrics, ABS, and aluminum in upholstery and interior trim applications. :contentReference[oaicite:0]{index=0}
Key Features
- Fast-drying nitrile adhesive provides high initial bond strength with excellent green strength.
- Resistant to solvents and plasticizer migration for durable flexible PVC assemblies.
- High-viscosity formulation supports brush, roll, or pre-application processes.
- Forms a clear, flexible, non-staining bond suitable for upholstery and interior trim applications.
Applications / Suitable For
- Flexible PVC to PVC bonding
- Plastic upholstery assembly
- Vinyl bonding
- PVC foam bonding
- Fabric laminating
- Bonding ABS and aluminum components
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Additional Information
As-Supplied / Before-Processing Properties
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Product type | One-part solvent-based nitrile adhesive | — | Supplier classification |
| Appearance | Amber liquid | — | Typical physical property |
| Total solids | 26 | % | Typical physical property |
| Specific gravity | 0.87 | — | Typical physical property |
| Thermosel viscosity | 2,250 | cP | Typical physical property |
| Flash point | -17 | °C | Typical physical property |
| Heat resistance | 65.6 | °C | Typical physical property |
| Shelf life | Approximately 9 months | — | Stored at 13–32°C in original sealed container |
After-Processing / Final-State Properties
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Bond appearance | Clear, flexible, non-staining film | — | After solvent evaporation |
| Green strength | Excellent | — | Supplier classification |
| Chemical resistance | Resistant to solvents and plasticizer migration | — | Supplier description |
| Typical bond strength (Fabric/Fabric) | 18–20 | pli | Typical bond values |
| Typical bond strength (Fabric/Vinyl) | 16–18 | pli | Typical bond values |
| Typical bond strength (Vinyl/Vinyl) | 16–18 | pli | Typical bond values |
| Typical bond strength (Vinyl/ABS) | 18–22 | pli | Typical bond values |
| Typical bond strength (Vinyl/Aluminum) | 18–22 | pli | Typical bond values |
| Vinyl Foam/Solid Vinyl | Foam failure | — | Typical bond value |