LOCTITE ABLESTIK NCA 2350
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other
Main features
- Fast cure
- Good adhesion
- Heat sensitive components
Product Description
LOCTITE ABLESTIK NCA 2350 is a non-electrically conductive epoxy adhesive, designed for use in heat-sensitive devices such as camera module housing assemblies.
LOCTITE ABLESTIK NCA 2350 is a high-performance epoxy adhesive that provides excellent thermal conductivity, adhesion, and chemical resistance. It is commonly used in microelectronics and semiconductor applications where thermal management is critical.
Cure Schedule
- 2 minutes @ 80 °C in hot plate
- 30 minutes @ 80°C in conventional oven
Packaging
Please select Package Type.
TDS, SDS & Technical Documents
Technical Specifications
Thermal Properties
Glass Transition Temperature (Tg)
28 °C The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding.
The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
Physical Properties
Thixotropic index
3.7 Thixotropic Index is a ratio of a material s viscosity at two different speeds in Ambient temperature, generally different by a factor of ten.
A thixotropic material s viscosity will decrease as agitation or pressure is increased. It indicates the capability of a material to hold its shape. Mayonnaise is a great example of this. It holds its shape very well, but when a shear stress is applied, the material easily spreads.
It helps in choosing a material in accordance to the application, dispense method and viscosity of a material.
Viscosity
13,670 mPa.s Viscosity is a measurement of a fluid’s resistance to flow.
Viscosity is commonly measured in centiPoise (cP). One cP is defined as
the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP.
A product like honey would have a much higher viscosity -around 10,000 cPs-
compared to water. As a result, honey would flow much slower out of a tipped glass than
water would.
The viscosity of a material can be decreased with an increase in temperature in
order to better suit an application
Mechanical Properties
Elongation
110 % Elongation is the process of lengthening something.
It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks.
It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.