LOCTITE ABLESTIK NCA 2286
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

Main features
- Dual Cure
- High elongation strength
- Active alignment in lens holder attach
Product Description
LOCTITE ABLESTIK NCA 2286 dual cure acrylic adhesive is designed for use in active alignment applications in camera module assembly. It has been formulated to a high viscosity and thixotropy to enable higher aspect ratios of dispensed adhesive, thus allowing for easier adjustments for the final assembly. This material jas a very high dispense aspect ration and is engineered to meet the high reliability performance requirements for the optoelectronic / semiconductor industry.
LOCTITE ABLESTIK NCA 2286 is black in color to prevent light penetration into the final assembled device. It is designed to achieve fast cure response at low temperatures and good depth of cure after UV radiation. This product also contains a secondary thermal cure mechanism for applications with shadowed areas where light is unable to penetrate. It is a camera/sensor market material that is not expected to pass very harsh reliability requirements.
Cure Schedule
UV Light
- UV Wavelength, nm 220 to 380
- Light Intensity, mW/cm² 1,000
- Exposure Time, seconds 4
Secondary Heat Cure
- 1 hour @ 80°C
TDS, SDS & Technical Documents
Technical Specifications
Thermal Properties
Mechanical Properties
Physical Properties
Additional Information
LOCTITE ABLESTIK NCA 2286 epoxy acrylate has, proven, good adhesion on glass and metals (see test data on 3x3mm glass die on difficult to bond nickel substrate below)