The dicing process is an intricate and crucial step during semiconductor manufacturing. During the dicing process, a high-speed saw (or laser) cuts through the wafer, cutting it into smaller pieces called dies.

The first part of the process is to mount the wafer to a stand with a dicing tape. Then, the wafer can be separated into dies. There are multiple methods to do this, but the most popular are blade or laser dicing.
Blade Dicing
The blade dicing method consists of a fast-moving, diamond coated blade that very quickly slices through the wafer. The cuts are extremely precise and smooth. Even though the process is very efficient, its main disadvantage comes to play with thinner and more fragile wafers. The blade can cause mechanical stress and chipping.
Laser Dicing
Laser dicing is a no-contact method of slicing the wafer. It uses laser technology to quickly cut the wafer into dies and is great for thin, fragile wafers that are complex. It is higher precision compared to blade dicing and reduces the mechanical stress that comes into play with the contact of the blade and the wafer. It also has less debris than the blade dicing process. However, it is a more expensive investment and, in some cases, can cause heat damage to the wafer.
Plasma Dicing
Another no-contact method of dicing is plasma dicing. It involves using plasma technology to slice the wafer. The high-energy plasma beam etches the wafer material. This method is ideal for applications which require no mechanical stress and is highly effective for cutting both brittle and complex wafers. It is even more expensive than laser dicing, however, is an extremely quick process and has no mechanical damage at all.
| Method | Blade | Laser | Plasma |
| Speed | good | better | best |
| Mechanical Damage | some damage | some damage | no damage |
| Debris | debris | no debris | no debris |
One of the most critical components during both the blade and laser dicing processes are dicing tapes. Dicing tapes are specialized tapes designed for use during the dicing process. They are thin, flexible, and have a strong adhesion layer.
The tape's main goals are to:
- Support the wafer - the tape holds the wafer securely, which means it won't move and thus won't be damaged by the blade during the cutting process.
- Be easily removable - since the tape isn't a part of the final component, it needs to be removed. After the removal of the tape the individual dies must remain intact and free of any residue.

.png)
UV Removable vs Non-UV Removable Dicing Tapes
UV Removable Dicing Tapes are widely used in dicing tapes to prevent the adhesion of residue to the wafer. When UV Light is applied, the adhesive becomes less tacky and allows for easy removal. This works because of the adhesive. The adhesive used is sensitive to UV light, and when exposed to it, it chemically alters to lose its bonding strength. One of the most important qualities of this technology is that no residue is left on the substrate. This makes it ideal for wafers.
Non-UV Removable Dicing Tapes are removed the traditional way. They are also specifically designed to leave no residue behind, however are more challenging to remove than a UV Removable Tape. They can be used in applications in which a consistent level of adhesion is needed. Non-UV Removable is a more economical option and is ideal for very fragile and thin dies that require strong adhesion throughout the entire process.
UV Removable Dicing Tapes need to meet these two performance requirements:
STRONG ADHESION STRENGTH BEFORE UV
The dicing tape must have a very high adhesion strength when initially placed on the wafer, to keep it secure during the slicing process.
WEAK ADHESION STRENGTH AFTER UV
After UV is applied, the adhesion strength must be weak to facilitate the easy removal from the individual dies.
Questions to ask when Choosing a Dicing Tape
✅ What is the adhesion strength required?
✅What is the adhesion strength required when removing the tape?
✅What is the thickness of the wafer?
✅What type of film is required for the process? (PET, Polyolefin, Polymerized Vinyl Chloride)
✅Does the process require UV Removable adhesive?
✅What are the operating conditions?
| Product | Adhesion Strength (Before UV) | Adhesion Strength (After UV) |
|---|---|---|
| DCT-PET115 | 19,000 | 100 |
| DCT-PO165 | 18,600 | 180 |
| DCT-PO200 | 23,000 | 200 |
| DCT-PVC95 | 3,200 | 140 |
⚡ Applications
▪ Dicing process
▪ Packaging substrates
✅ Advantages
✔ Strong adhesion to prevent substrate damage
✔ Quick removal with UV Removable technology
✔ Withstands mechanical stress and pressure variations, ensuring long-term durability
📥 Downloads
⬇
LINQTAPE DICING Tapes for Semiconductor Wafers
Since the dicing process is an extremely sensitive application, the tapes require specialized materials. LINQTAPE PET, Polyolefine, and Polymerized Vinyl Chloride Dicing Tapes are designed specifically to meet these needs, offering excellent mechanical strength and high adhesion without residue.

LINQTAPE DCT-PET115 is a transluscent polyethylene terephthalate (PET) tape designed for the dicing process. It provides an excellent balance of electrical, mechanical, thermal, and chemical properties.

LINQTAPE Polyolefin Dicing Tapes feature the same strong adhesion as the PET Series but are more easily removed from the substrate. This makes it ideal for applications such as packaging substrates or delicate substrates where gentler adhesion is required for easier removal. Polyeolefin Dicing tapes are available in two thicknesses, 165 μm (DCT-PO165) and 200 μm (DCT-PO200)

LINQTAPE Polymerized Vinyl Chloride Dicing Tapes offer superior mechanical strength and excellent adhesion while being easy to remove without residue. These tapes are transparent, UV Removable, and ideal for high-precision applications. PVC Dicing Tapes are available in 80 μm (DCT-PVC80NUV), and 95 μm (DCT-PVC95) thicknesses.