Water Electrolyzers

Alkaline, PEM and AEM Electrolyzers

PEM Electrolyzers

 


In a stark contrast to alkaline water electrolyzers (ALK WEs) proton exchange membrane water electrolyzers (PEMWEs) use a solid polymer electrolyte membrane (also known as ion exchange membrane) instead of a liquid electrolyte to split ultra-pure water into hydrogen and oxygen.

The limitations of ALK WEs have driven significant innovation in electrolyzer stack designs; most notably, the development of solid polymer electrolyte membranes, also known as ion exchange membranes. These proton-conducting membranes were originally developed in the 1960s for fuel cell applications (see: proton exchange membranes for fuel cells) and played a key role in early space exploration missions. Over the decades, their design and performance have been refined, making them suitable for electrolysis applications as well.

 

Water Electrolyzer Technology Advancement Timeline

Advancements in Water Electrolyzer Technology: From Alkaline to PEM Systems

 

Innovations in water electrolyzer technology have emerged to address the limitations of the first-generation alkaline water electrolyzers. A major turning point came in the 1960s with the invention of proton exchange membranes (PEMs), which paved the way for PEM electrolyzers. These newer systems offered improved performance, higher current densities, and more compact designs.


How do PEM Water Electrolyzers Work?

Hydrogen and oxygen gases are produced on either sides of the membrane and are removed from the back of the electrodes through suitable cathode gas diffusion layers and anode porous transport layers. PEMWEs operate under highly acidic conditions (pH <2), where water splitting occurs through the following half-reactions:

  • At the anode, water molecules are oxidized, producing oxygen gas, protons (H⁺), and electrons: H2O (l) → 2 H+ (aq) + ½ O2 (g) + 2 e
  • At the cathode, protons (H⁺) are reduced, producing hydrogen gas: 2 H+ (aq) + 2 e → H2 (g)
A diagram illustrating the anode and cathode reactions in a PEM water electrolyzer

Cathode Reactions in Proton Exchange Membrane Water Electrolyzers

Anode Reactions in Proton Exchange Membrane Water Electrolyzers

 


PEM Water Electrolyzer Components

Labeled diagram of a PEM water electrolyzer showing key components including the proton exchange membrane, anode and cathode catalyst layers, porous transport layers, bipolar plates

PEM water electrolyzers consist of several key components that work together to enable efficient hydrogen production: a proton exchange membrane, catalysts, cathode gas diffusion layer (GDL), and anode porous transport layer (PTL). Each layer is engineered to support water management, gas diffusion, and electrochemical performance under highly acidic and pressurized operating conditions.

In addition to the membrane-electrode assembly (MEA), balance of stack components such as flat gaskets, bipolar plates, and cell frames ensure proper sealing, electrical conductivity, and structural support across the stack.

Proton Exchange Membranes

An ion exchange membrane (IEM) is a thin barrier that allows the selective passage of ions from one electrode to another of electrochemical devices. In PEM water electrolyzers, a proton exchange membrane (also called a proton-conducting membrane) enables the transport of H⁺ ions from the anode—where they are generated—to the cathode, where they are consumed.

More importantly, proton exchange membranes keep the anode and cathode physically separated, preventing the mixing of H₂ and O₂ product gases. This is a crucial safety feature—just 4.6% oxygen in a hydrogen stream or 3.8% hydrogen in an oxygen stream is enough to form an explosive mixture at 80 °C, which is close to the typical operating temperature of water electrolyzers.



Anode and Cathode Catalyst Layers (Catalyst + Ionomer)

Catalysts speed up reactions without being consumed in the process. In water electrolyzers, catalysts enable reactions that generate H2 and O2 gases to happen efficiently at practical input voltage.

In PEM water electrolyzers, the cathode catalyst speeds up the hydrogen evolution reaction (HER). On the other side, the anode catalyst drives the oxygen evolution reaction (OER). These catalysts are typically noble-metal-based due to the harsh, acidic environment of PEM systems. Platinum is the most commonly used catalyst at the cathode because of its excellent HER activity and durability. At the anode, iridium oxide or ruthenium oxide is used for OER.

Illustration showing anode and cathode catalyst layers in a PEM water electrolyzer


Catalysts are usually in powder form.  How do we actually use them in electrochemical devices like PEM water electrolyzer stacks? It all starts with an ink.

This catalyst ink is a mixture of the powdered catalyst, a solvent (like water or alcohol), and an ionomer or a polymer that conducts protons and helps bind the catalyst particles to the membrane or gas diffusion layer. The ink is applied as a thin coating, typically through spraying, printing, or brushing, to create what’s called a catalyst layer. Once dried and properly processed, this layer becomes an integral part of the membrane electrode assembly (MEA), where the electrochemical reactions take place.

Catalyst ink components: solid catalyst particles and ionomer in a solvent
Catalyst ink components: solid catalyst particles and ionomer in solvent
Coating catalyst ink onto a membrane or gas diffusion layer
Coating catalyst ink onto membrane or gas diffusion layer
Gas Diffusion Electrode (GDE) vs Catalyst-Coated Membrane (CCM)
GDE vs CCM: Catalyst layer on backing vs directly on membrane

Pemion PP1-HNN8-00 Ionomer for PEMWE Catalyst Inks

PEMION® PP1-HNN8-00 Ionomer is a high-performance proton exchange ionomer designed for use in PEM water electrolyzers and fuel cells. It offers excellent proton conductivity, chemical stability in acidic environments, and superior film-forming properties, making it ideal for catalyst ink formulations and membrane electrode assemblies (MEAs).

 

Ionomer Type IEC (meq/g) EW (g/eq.) Density (g/cm³) Solubility
PP1-HNN8-00 2.8 - 3.1 320 – 360 1.2 Alcohols and alcohol/water mixtures
Ionomer Type (reference)
Long side-chain PFSA
(for reference only)
0.9 - 1.0 1000 – 1,100 2.0 Alcohols and alcohol/water mixtures
Short side-chain PFSA
(for reference only)
1.1 - 1.3 770 – 910 2.0 Alcohols and alcohol/water mixtures

Applications

  • Catalyst ink formulations for PEM water electrolyzers
  • Membrane Electrode Assemblies (MEAs) in fuel cells

Advantages

✔ High proton conductivity for efficient ion transport

✔ Excellent chemical stability under acidic and oxidative conditions

✔ Superior film-forming capability for uniform catalyst layers


Cathode Gas Diffusion Layers and Anode Porous Transport Layers

Diagram illustrating the roles of gas diffusion layers (GDLs) at the cathode and porous transport layers (PTLs) at the anode in a PEM water electrolyzer stack

Porous transport layers (PTLs) and gas diffusion layers (GDLs) are important components in water electrolyzer stacks. They play several key roles:

Reactant feed and product removal

They help water reach the catalyst and allow hydrogen and oxygen to escape. Poor gas removal limits water supply and can reduce performance.

Electron transport

PTLs and GDLs carry electrons between the catalyst layer and the bipolar plate for efficient hydrogen production.

Heat management

They help spread and release heat to prevent hot spots and membrane damage.

 

The choice of material to be used at the anode and cathode depends on the operating environment and requirements at each electrode.

Side Layer Typical Material Operating Conditions Reason
Cathode Gas Diffusion Layer (GDL) Carbon ~0 V vs. RHE, reducing environment, acidic pH (0–1) Stable under reducing conditions, good conductivity, and cost-effective
Anode Porous Transport Layer (PTL) Titanium ~1.6–2.0 V vs. RHE, oxidizing environment, acidic pH (0–1) Excellent corrosion resistance under acidic and oxidative conditions
 

Find a more in-depth explanation of material choices and their performance in water electrolyzer stacks in

LINQCELL Graphitized Carbon Fiber Panels as PEMWE Cathode GDLs

LINQCELL Graphitized Carbon Fiber Plates are made by layering carbon fibers or particles with a conductive binder. KRAYDEN's carbon fibers are made from polyacrylonitrile fibers, which are then graphitized by heating the material to high temperatures in an inert atmosphere to convert it into graphite. These are thicker versions of carbon fiber papers.

 

Featured Products

LINQCELL GDL1500
1.5 mm thickness
  • 1.5mm - 1500 um - 59mil
  • Alternative to Spectracarb 6060
  • Also available in a more compressible version (GDL1500B)
LINQCELL GDL1850
1.85 mm thickness
  • 1.85mm - 1850 um - 73mil
  • Alternative to Spectracarb 7590
LINQCELL GDL2900
2.9 mm thickness
  • Thickest graphitized carbon fiber plate
  • Basis weight can be as high as 1800 g/m2
  • Low voltage loss (27 mV)

 

Key Features and Benefits of LINQCELLTM Graphitized Carbon Fiber Panels 

  • Low resistance, which minimizes energy losses and improves overall fuel cell efficiency
  • Customizable GDL solutions to meet specific performance needs
  • High corrosion resistance, making them durable in acidic conditions of fuel cells
  • High mechanical strength, critical for maintaining integrity under high-pressure conditions
  • Customizable compressibility

LINQCELL Sintered Titanium as PEMWE Anode PTLs

Titanium is the preferred material for the anode porous transport layers (PTLs) of PEM water electrolyzers due to its excellent corrosion resistance in the highly oxidative and acidic environment on the anode side. It forms a stable oxide layer that protects against degradation while maintaining mechanical strength and stability under pressure and temperature.

LINQCELL™ Sintered Titanium Fiber Felts are produced from titanium wires drawn to a micron-scale diameter. These wires are stacked using a specialized laying method, then subjected to pressure and placed in a high-temperature vacuum environment for sintering. This fuses the nodes between fibers, forming a three-dimensional network structure.

LINQCELL™ Sintered Titanium Fiber Felts
  • Grades: Ta0 (≥99.9% purity), Ta1 (Grade 1), Ta2 (Grade 2)
  • Porosity: 50–80%
  • Thickness: 0.20 mm – 1.5 mm
  • Fiber diameter: 20–25 μm
  • Max dimensions: 120 cm × 120 cm
  • Optional platinum coating: Both sides, up to 0.50 μm

Also available: LINQCELL Sintered Titanium Powder


Frequently Asked Questions about PEM Water Electrolyzers

What are PEM electrolyzers used for?

PEM electrolyzers are used for producing high-purity hydrogen in applications such as green hydrogen generation, hydrogen fueling stations, power-to-gas systems, synthetic fuel production, and industrial gas supply. Their dynamic response and compact design make them ideal for renewable energy integration.

What water quality is required for PEM electrolyzers?

PEM electrolyzers require deionized water with a resistivity ≥1 MΩ·cm. Poor water quality can lead to membrane degradation, catalyst poisoning, and loss of efficiency, so high-purity water is essential for reliable operation.

What’s the difference between PEM and AEM electrolyzers?

PEM electrolyzers use acidic membranes and require noble metal catalysts like iridium and platinum. AEM electrolyzers operate in alkaline conditions and can use non-precious metals. PEM systems are more mature, with higher performance, while AEM offers potential for lower cost but is still emerging.

Can PEM electrolyzers operate intermittently?

Yes. PEM electrolyzers have fast ramp-up times and excellent dynamic response, allowing them to efficiently operate under fluctuating power input from renewable energy sources like solar or wind.

Materials for PEM Water Electrolyzers

Curious about how the right materials can improve electrolyzer performance? This presentation showcases KRAYDEN's material solutions for PEM water electrolyzers, highlighting their composition, performance characteristics, and ideal applications. Discover how these advanced materials enhance efficiency, improve durability, and support reliable hydrogen production in demanding PEM electrolyzer systems.

Types of Low-Temperature Electrolyzers

The presentation shown on the right introduces the main types of low-temperature electrolyzers—systems that operate below 150 °C and are widely used for green hydrogen production. It explores alkaline, PEM, and AEM electrolyzers, explaining their operating principles, key materials, advantages, and technical challenges to help readers understand the strengths and trade-offs of each technology.

Related Blogs

Differences Between Alkaline, PEM, and AEM Water Electrolyzers

What are the Differences Between Alkaline, PEM, and AEM Water Electrolyzers?

This blog explores the key differences between alkaline, PEM (proton exchange membrane), and AEM (anion exchange membrane) water electrolyzers. It breaks down how each technology works, compares their materials and operating conditions, and highlights their respective advantages and limitations.

Differences Between Sintered Metal Powders and Sintered Metal Fiber Felts

What Are the Differences Between Sintered Metal Powders and Sintered Metal Fiber Felts?

This blog explores the differences between sintered metal powders and sintered metal fiber felts, focusing on their structure, permeability, and performance in various applications. It also provides insights into the structure of sintered nickel fibers, helping readers understand what makes them suitable for alkaline water electrolyzers.

Impending PFAS-ban Affect Proton Exchange Membranes for Water Electrolyzers and Fuel Cells

How Will the Impending PFAS-ban Affect Proton Exchange Membranes for Water Electrolyzers and Fuel Cells?

This blog discusses the potential impact of the impending PFAS ban on proton exchange membranes (PEMs) used in water electrolyzers and fuel cells. It examines why PFAS-based materials have been widely used, what challenges the ban presents for current membrane technologies, and how the industry is responding with PFAS-free alternatives.

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers