PERMABOND LM113
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

Main features
- Low-Strength Easy-Disassembly Threadlocking
- Medium-Viscosity Non-Drip Application
- MIL-S-46163A/ASTM D5363 Compliance
Product Description
Permabond® LM113 is a medium-viscosity, low-strength anaerobic threadlocker specifically designed for securing small threaded fasteners, screws, bolts, and hydraulic fittings that may require future disassembly. Formulated as a PFAS-free, 100% solid liquid, it cures rapidly at room temperature when confined between metal parts, providing excellent protection against vibration-induced loosening. Its thixotropic properties ensure the adhesive remains precisely where applied without running, while also lubricating the threads to facilitate easier initial assembly.
Key features
- Low strength for disassembly: Provides a controlled off-torque (Breakaway 9 N-m), allowing for easy maintenance and disassembly of small or delicate fasteners.
- Thixotropic rheology: The medium viscosity (1,200 cP) and thixotropic nature prevent the adhesive from dripping or migrating away from the application area.
- Military and ASTM approved: Meets the strict lot testing requirements of military specification MIL-S-46163A (Type II Grade M) and ASTM D5363 (AN 0311 Group 03 Class 1 Grade 1).
Applications / Suitable for
- Locking and sealing small threaded fasteners, screws, bolts, and hydraulic fittings (up to M20 / 3/4")
- Assemblies requiring protection against vibration loosening and corrosion
- Applications requiring controlled, low-strength locking for future disassembly and maintenance
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Other Properties
Electrical Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical Composition | Methacrylate esters | - | - |
| Appearance | Purple / Violet | - | Liquid |
| Viscosity | 1,200 | mPa.s (cP) | at 25°C (Thixotropic) |
| Specific Gravity | 1.1 | - | - |
| Maximum Gap Fill | 0.15 | mm | (0.006 in) |
| Maximum Thread Size | M20 | - | (3/4") |
| Flash Point | > 100 | °C | (212°F) |
After-processing / final-state properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Handling Strength Time | 15 | minutes | M10 steel at 23°C |
| Full Strength Time | 24 | hours | M10 steel at 23°C |
| Breakaway Torque Strength | 9 | N-m | M10 steel (ISO 10964) (80 in.lb) |
| Prevailing Torque Strength | 5 | N-m | M10 steel (ISO 10964) (40 in.lb) |
| Shear Strength | 5 | MPa | Steel collar & pin (ISO 10123) (750 psi) |
| Coefficient of Thermal Expansion | 90E-6 | mm/mm/°C | - |
| Dielectric Strength | 11 | kV/mm | - |
| Thermal Conductivity | 0.19 | W/(m.K) | - |