    Product Description

    Permabond® 910FS Cyanoacrylate is a 100% reactive, methyl-based cyanoacrylate adhesive designed for rapid, high-strength bonding. As the original 100% methyl cyanoacrylate, this solvent-free, low-viscosity liquid cures incredibly fast at room temperature when pressed into a thin film. It is specifically engineered to provide exceptional adhesion to metals—such as steel, aluminum, brass, and stainless steel—while also effectively bonding a wide variety of plastics and rubbers.

    Key features

    • Extremely fast setting: Rapidly develops high strength without mixing or heat curing, achieving fixture times of under 5 seconds on steel.
    • Excellent metal adhesion: Specially designed to provide superior bond strength (up to 4200 psi) on a variety of metal surfaces.
    • Industry approved: Meets rigorous specifications, including approval to MIL-A-46050C Type I Class 1 for existing designs and CID A-A-3097 Type I Class 1 for new designs.

    Applications / Suitable for

    • High-strength bonding of metals, including steel, aluminum, and brass
    • Bonding various plastics and rubbers
    • High-speed assembly requiring rapid fixture times
    Product Family

    PERMABOND 910FS

    Catalog Product

    Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

    TDS, SDS & Technical Documents

    Technical Specifications

    General Properties
    AppearanceAppearance
    Liquid
    Chemistry TypeChemistry Type
    Methyl cyanoacrylate
    ColorColor
    Colourless
    Specific GravitySpecific Gravity
    1.1
    Physical Properties
    ViscosityViscosity
    2-4 mPa.s mPa.s
    Mechanical Properties
    Impact StrengthImpact Strength
    3-5 kJ/m² mm
    Linear thermal expansionLinear thermal expansion
    90 x 10^-6 mm/mm/°C
    Thermal Properties
    Thermal ConductivityThermal Conductivity
    0.1 W/m.K
    Electrical Properties
    Dielectric StrengthDielectric Strength
    25 kV/mm
    Maximum gap fillMaximum gap fill
    0.05 mm

    Additional Information

    Technical properties

    As-supplied / before-processing properties

    Typical properties; these values are not intended for use in preparing specifications.

    Property Value Unit Method / condition
    Chemical Composition Methyl cyanoacrylate - -
    Appearance Colorless - Liquid
    Viscosity 2-4 cP at 25°C (mPa.s)
    Specific Gravity 1.1 - -
    Maximum Gap Fill 0.05 mm (0.002 in)
    Flash Point 83 °C (181.4°F)
    Technical properties

    After-processing / final-state properties

    Typical properties; these values are not intended for use in preparing specifications.

    Property Value Unit Method / condition
    Fixture/Handling Time < 5 seconds Steel
    Full Strength 24 hours -
    Shear Strength 23-29 N/mm² Steel (ISO 4587) (3300-4200 psi)
    Impact Strength 3-5 kJ/m² ASTM D-950 (1.4-2.4 ft-lb/in²)
    Hardness 85 Shore D ISO 868
    Dielectric Constant 2.5 - at 10kHz
    Dielectric Strength 25 kV/mm -
    Coefficient of Thermal Expansion 90E-6 mm/m/°C -
    Coefficient of Thermal Conductivity 0.1 W/(m.K) -

    Leading Brands Trust in Our Products and Services

    • Jabil
    • Linxens
    • Magna
    • Medtronic
    • NXP
    • Philips
    • Semikron
    • Teledyne
    • Thales
    • Vishay
    • ZF
    • AMS
    • Apple
    • Audi
    • Broadcom
    • Borgwarner
    • Bosch
    • Eaton
    • Henkel
    • Honeywell
    • Hysol
    • Intel
    Products that Perform|Knowledge that Serves|Service that Delivers