MP 55305
Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses
Main features
- No-Prep Impact-Resistant Bonding
- 2 to 3-Minute Open Time
- Thermal-Cycling and Chemical Resistance
Product Description
MP-55305 is a high-performance, two-part structural methyl methacrylate (MMA) adhesive designed for bonding a wide range of materials, including plastics, metals, and composites. It cures at room temperature and delivers exceptional strength and stiffness with outstanding resistance to temperature fluctuations, thermal cycling, and harsh chemicals without requiring surface preparation.
Key features
- No surface preparation required: Ensures long-lasting reliability and high impact resistance without the need to prepare most surfaces.
- Fast curing and convenient: Features a 1:1 mix ratio with a 2 to 3 minute open time and achieves fixture in 5 to 8 minutes at room temperature.
- UL Certified: Recognized as a component for sign accessories under file number E350958.
Applications / Suitable for
- Suitable for bonding metals such as aluminum, steel, stainless steel, and e-coated metal.
- Designed for thermosets including fiberglass, phenolic, epoxy, and polyurethane.
- Ideal for thermoplastics like acrylic, ABS, polycarbonate, PVC, and nylon/PA.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Appearance
Amber or green, viscous liquid Appearance at room temperature.
Mix Ratio
1:1 The amount of a constituent divided by the total amount of all other constituents in a mixture
Pot Life
2–3 min minutes Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed.
It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
Product Type
Two-part modified acrylic structural adhesive Material category or functional product class.
Additional Information
Technical properties
As-supplied / before-processing properties
Pre-cure properties of MP-55305 structural adhesive.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance / Color | Amber or Green | - | - |
| Mix Ratio (Volume & Weight) | 1:1 | - | - |
| Viscosity (Resin) | 60,000-80,000 | cPs | Brookfield RV7, 20 RPM, 25°C |
| Viscosity (Activator) | 60,000-120,000 | cPs | Brookfield RV7, 20 RPM, 25°C |
| Mixed Density | 0.98 | g/cc | - |
| Open Time | 2-3 | Minutes | - |
| Fixture Time | 5-8 | Minutes | - |