Main features
- Metal-Free Anti-Seize Formulation
- 4,800 N Weld Load
- Controlled M12 Fastener Friction
Product Description
MOLYKOTE P-74 Assembly Paste is a grayish-black, PAO-based, metal-free assembly paste with graphite and white solid lubricants for anti-seize and lubricating applications. The paste carries a typical 4,800 N four-ball weld load and has a service range of -40 to 200 deg C; selected raw materials continue to act as separating agents at 1,500 deg C in the dry-lubricant state. Applications include bolted connections, sliding bearings, linear guides, splined shafts, press-fit joints, exhaust and spark-plug threads, flanges, hinges, and brake mechanisms.
Key features
- Metal-Free Anti-Seize Formulation: PAO base oil is combined with graphite and white solid lubricants without metallic solids.
- 4,800 N Weld Load: The four-ball weld-load result is measured by DIN 51350, Part 4.
- Controlled Fastener Friction: An M12 grade 8.8 test produced 0.14 thread and 0.08 head friction coefficients.
Applications / Suitable for
- Bolted and threaded connections.
- Sliding bearings, linear guides, and splined shafts.
- Press-fit joints, flanges, hinges, and brake mechanisms.
- Exhaust bolts and spark-plug threads.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Additional Information
As-supplied paste properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Grayish black | Typical | |
| Physical form | Paste | Typical | |
| Unworked penetration | 280 to 310 | mm/10 | CTM 191; typical |
| Density | 1.21 | g/ml | At 20 deg C; typical |
In-service performance properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Paste service-temperature range | -40 to 200 | deg C | Typical |
| Dry-lubricant separation function | 1,500 | deg C | Selected raw materials continue to act as separating agents |
| Four-ball weld load | 4,800 | N | DIN 51350, Part 4; typical |
| SRV oscillating wear duration | 90 | min | 300 N, 1,000 um, 20 Hz at 90 deg C; typical |
| Thread/head friction coefficient | 0.14 / 0.08 | CTM 1153, M12 grade 8.8 blackened surface; typical | |
| Press-fit friction coefficient | 0.12 | CTM 394; typical | |
| Salt-spray duration | 140 | h | ISO/R 1456 at 50 um coating thickness; typical |
| Emcor corrosion degree | 2 | DIN 51802; typical |