LOCTITE EDAG 1415M
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

Main features
- Silver-Filled Coating Application
- Low-Resistance Coating Application
- No Primer or Topcoat Required
Product Description
LOCTITE® EDAG 1415M E&C is a silver-filled thermoplastic conductive coating developed to provide electromagnetic compatibility (EMC) and EMI shielding protection for electronic equipment enclosures. The coating is compatible with many engineering plastics and delivers low surface resistance, high attenuation performance, and excellent environmental durability without requiring a primer or top coat. It can be applied by spray or brush and air dries rapidly for efficient production processing.
Key Features & Benefits
- Silver-filled thermoplastic conductive coating.
- Designed for EMC and EMI shielding applications.
- Maintains low resistance after environmental exposure.
- No primer or top coat required.
- Suitable for spray or brush application.
- Fast air-dry processing with optional forced drying.
- Compatible with plastics used in electronic enclosures.
Recommended Applications
- EMI shielding of plastic electronic housings.
- EMC compliance coatings.
- Electronic equipment enclosures.
- Conductive coating applications requiring low resistance.
- Industrial electronic assemblies and housings.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Thermal Properties
Additional Information
As-Supplied / Before-Processing Properties
| Property | Value | Unit | Condition |
|---|---|---|---|
| Technology | Thermoplastic Conductive Coating | — | Silver-filled EMC coating |
| Appearance | Silver | — | As supplied |
| Solids Content | 58 | % | Typical |
| Viscosity | 375 | mPa·s (cP) | Brookfield, 20°C, 20 rpm |
| Density | 1,630 | kg/m³ | Typical |
| Theoretical Coverage | 9 | m²/kg | 10 μm coating thickness |
| Shelf Life | 18 | months | 5 to 30°C storage |
| Flash Point | 14 | °C | Typical |
| Operating Temperature | 105 | °C | Maximum service temperature |
After-Processing / Final-State Properties
| Property | Value | Unit | Condition / Method |
|---|---|---|---|
| Recommended Coating Thickness | 10 - 15 | μm | For EMI shielding performance |
| Attenuation | 60 | dB | 1,000 MHz, 25 μm thickness |
| Sheet Resistance | <0.015 | Ω/sq | 25 μm coating thickness |
| Dry to Touch Time | 10 | minutes | Ambient conditions |
| Handling Time | 20 | minutes | Approximate |
| Air Dry Time | 4 - 8 | hours | Good coating properties achieved |
| Recommended Drying Cycle | 30 min @ 70-80 | °C | Forced drying improves conductivity |
| Spray Pressure | 2.0 - 2.5 | bar | Recommended application setting |
| Nozzle Diameter | 1.0 - 1.5 | mm | Spray application |