LOCTITE EA 9895
Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

Main features
- One-Piece Peel-Ply Removal
- Bond-Ready Surface Without Sanding
- 177 deg C Prepreg Co-Cure
Product Description
LOCTITE EA 9895 WPP AERO is a one-part polyester wet peel ply film for preparing composite bond surfaces during co-cure. The off-white film has a nominal areal weight of 161 g/m^2, 48% resin content and a polyester peel-ply carrier. After cure and removal, it leaves a clean surface ready for the next bonding step without sanding or solvent wiping. The fabric strips in one piece, supporting efficient processing on large composite parts. The film cures for 90 to 120 minutes at 177 deg C and is compatible with composite prepreg resin systems.
Key features
- One-piece peel removal: The cured fabric strips in one piece to reduce removal time.
- Bond-ready surface: Removal leaves a clean surface ready for the next bonding step without sanding or solvent wiping.
- Prepreg co-cure processing: The film cures at 177 deg C and is compatible with composite prepreg resin systems.
Applications
Applications include composite bond-surface preparation and wet peel-ply processing with compatible composite prepreg resin systems.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Other Properties
Additional Information
As-supplied properties
Product details for the one-part wet peel ply film.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product form | One-part film | Wet peel ply | |
| Areal weight | 161 | g/m^2 | 0.033 lb/sf |
| Support carrier | Polyester peel ply | As supplied | |
| Roll dimensions | Nominal 1 m x 50.9 m | 3 ft x 167 linear ft | |
| Resin content | 48 | % | Nominal |
| Storage temperature | -18 or below | deg C | Cold storage |
| Open assembly time | At least 14 | days | At 25 deg C |
| Open assembly time | At least 7 | days | At 32 deg C |
Final-state properties
Characteristics after cure and peel-ply removal.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Removal behavior | Strips in one piece | After cure | |
| Bond-surface condition | Clean and ready for bonding | After fabric removal | |
| Residual polyester fibers | Minimal | After removal | |
| Additional surface preparation | Not required | No sanding or solvent wiping |