LOCTITE EA 9017
Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

Main features
- Premeasured Resin-Hardener Pack
- Fast 4-6-Minute Handling
- Machinable Cured Epoxy Finish
Product Description
LOCTITE EA 9017 is a two-component, room-temperature-curing epoxy adhesive supplied in a premeasured syringe pack for permanent bonding and repair. The clear water-white-to-amber liquid reaches handling strength in 4 to 6 minutes and full cure in 45 to 60 minutes. It bonds metals, ceramics, concrete, wood, glass and most plastics, while the cured material can be drilled, tapped, sanded, machined and painted. Applications include production, maintenance and prototype bonding, plus filling and sealing holes, cracks and worn surfaces.
Key features
- Premeasured syringe pack: Resin and hardener are supplied in measured quantities for consistent mixing and application.
- Fast handling and cure: Handling strength develops in 4 to 6 minutes, with full cure in 45 to 60 minutes.
- Machinable cured epoxy: The cured material can be drilled, tapped, sanded, machined and painted.
Applications
Applications include bonding metals, ceramics, concrete, wood, glass and most plastics, plus repairing, filling and sealing holes, cracks and worn surfaces.
Technical Specifications
No specifications available.
Additional Information
As-supplied properties
Typical uncured-product values.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical type | Epoxy and resin | Two-component system | |
| Appearance | Clear water-white to amber liquid | Uncured | |
| Specific gravity | 1.13 to 1.17 | Uncured | |
| Storage range | 8 to 28 | deg C | Unopened container in a cool, dry location |
Final-state properties
Typical cured-product values unless otherwise stated.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Cured appearance | Translucent | Fully cured material | |
| Shear strength | 2,300 | psi | ASTM D 1002 |
| Temperature resistance | Up to 149 | deg C | Cured adhesive |