LOCTITE EA 1C
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

Main features
- Multi-Material Metal/Plastic/Wood Bonding
- Machineable Sandable Cured Epoxy
- Low-Outgassing Epoxy Adhesive
Product Description
LOCTITE EA 1C is a two-part epoxy adhesive and sealant designed for bonding, sealing, and repair applications involving metals, most plastics, and wood. The system consists of an off-white resin and green hardener mixed at a 2.5:1 volume ratio and cures at room temperature after mixing, with optional heat curing to accelerate property development. The adhesive offers a combination of machinability, sandability, high service temperature capability, and low outgassing characteristics. After curing, it develops strong adhesion to aluminum substrates, good thermal conductivity, electrical insulation properties, and resistance to environmental exposure, making it suitable for demanding industrial assembly and repair applications.
Key features
- Low outgassing epoxy system: Exhibits low total mass loss and collected volatile condensable material after cure.
- Machineable and sandable: Supports finishing and post-cure modification of bonded or repaired components.
- High-temperature performance: Maintains measurable lap shear strength across a broad service-temperature range up to 149°C.
Applications / Suitable for
- General-purpose bonding of metals.
- Bonding and repair of most plastics.
- Wood bonding and repair applications.
- Sealing and gap-filling applications.
- Industrial maintenance and repair operations.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-Supplied / Before-Processing Properties
| Property | Value | Unit | Condition |
|---|---|---|---|
| Technology | Epoxy | — | Two-component system |
| Mix Ratio (Volume) | 2.5 : 1 | Resin : Hardener | As supplied |
| Mix Ratio (Weight) | 100 : 44 | Resin : Hardener | As supplied |
| Resin Specific Gravity | 1.63 | — | 25°C |
| Hardener Specific Gravity | 1.66 | — | 25°C |
| Resin Viscosity | 120,000 - 350,000 | mPa·s | Brookfield RV, 25°C |
| Hardener Viscosity | 500,000 - 900,000 | mPa·s | Brookfield RV, 25°C |
| Pot Life | ≥20 | minutes | 100 g mass @ 25°C |