PIT0.5S-UT-RL | 0.5-mil Polyimide (Kapton) Tape | Ultra-Thin Silicone Adhesive with Release Liner
Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

Main features
- 0.5 mil polyimide film
- Silicone adhesive
- >1500V breakdown voltage
Product Description
Ultra-Thin Pressure Sensitive Polyimide Tape
LINQTAPE™ PIT0.5S-UT Series tapes are our thinnest available high temperature tapes. It combines our 0.5-mil (13 micron) thick polyimide film – the generic equivalent of DuPont® Kapton™ HN tape – with an ultra-thin 0.5mil silicone pressure adhesive. This combination makes the PIT0.5S-UT-Series tapes our thinnest polymide products to date, with a total thickness of only 1 mil (25µm). Yet, it still has excellent adhesion and mechanical strength at high temperatures.
Ultra-Thin, Flame Retardant Polyimide Tape
LINQTAPE™ PIT0.5S-UT-Series tapes are high performance, temperature resistant polyimide tapes that use a polyimide film as a backing film. This backing film is the generic version of DuPont's Kapton HN film and is ultra-thin at 0.5mil (13µm) yet is just as flame retardant as its thicker counterparts. Laminated to this is a 0.5mil (13µm) thick pressure sensitive silicone adhesive making the total thickness of the polyimide film plus adhesive only 1mil (25µm) thick. PIT0.5S-UT Series remains both electrically and mechanically stable across temperatures ranging from -269°C to 400°C (-452°F to 752°F).
LINQTape HN Polyimide Film is Versatile
LINQTape HN Polyimide is available as a stand-alone film (LINQTape PIT0.5N Series) in standard thicknesses of 0.5 mil (13 micron), 1 mil (25 micron), 2 mil (50 micron), 3 mil (75 micron) and 5 mil (125 micron). It is also available with specialty coatings applied to the tape such as a conductive polymer to make it antistatic, a sputtered aluminum coating, corona resistant, with a FEP fluoropolymer coating, or as a black polyimide version. Custom thicknesses and/or coatings may be available, please ask for more details.
Once coated with the desired coating, it can be used as the backing film of many of our polyimide tapes which make it a pressure sensitive adhesive by applying either a silicone, rubber or acrylic adhesive layer. The adhesive layer is most often applied 1.5 mil (37 micron) thick, except in our thinnest product offerings which offers adhesive thicknesses as low as 0.5mil (13 micron) - this is our PIT0.5S-UT Series tapes. The adhesive may also be applied on one or both sides of the tape, and options are available to have it on a single or double-release, PET liner which makes it easier for handling or for the purpose of die-cut parts.
Product Applications
Polyimide tape is widely used in applications requiring high electrical insulation and an excellent balance of thermal, mechanical, chemical and electrical properties. As a base material, polyimide is extremely versatile as it can be die-cut, punched and thermoformed with or without adhesive.
It is extremely well suited, and extensively used for wrapping cable and magnet wire. A further list of applications includes, but is not limited to aircraft and spacecraft wiring, insulation tubing, slot insulation, fiber optics cable, heater circuits, automotive diaphragms and manifolds, high temperature splicing and other applications that can make use of the ultra-thin, high temperature, electrically insulating properties of the PIT0.5S-UT polyimide HN tapes.
Applications
- Cable Wrapping
- Magnet Wire Wrapping
- Automotive Manifolds
- Automotive Diaphragms
- Flexible Printed Circuits
- Heater Circuits
- Aircraft / Spacecraft Wiring
- Insulation Tubing
- Slot Insulation
- Fiber Optics Cable
- High Temperature Splicing
- 3D printing ABS plastic
Product Features and Benefits
- Good Chemical Resistance
- Mechanically and electrically stable from -269°C to 400°C (-452°F to 752°F)
- Can be laminated, die-cut, metallized, punched, adhesive coated and thermoformed
- Insensitive to radiation damage
- Adheres well to ABS
- Improved Moisure Barrier
Product Nomenclature
- PIT: HN Polyimide Tape
- 0.5: 0.5 mil (13µm) thick tape
- S: Silicone adhesive
- UT: Ultra-Thin Adhesive Layer
Technical Specifications
General Properties
Thermal Properties
Electrical Properties
Other Properties
Mechanical Properties
Additional Information
{tab=Pricing & Availability}
|
Volume Price Breaks can be seen for each product by clicking on its respective link under the DESCRIPTION column and looking to the volume price break table to the right of the product image. Price per unit is reflected in this table and used during checkout. KRAYDEN lists all its prices without taxes, shipping payment charges or discounts. KRAYDEN has entities in Canada and the Netherlands, and if your shipping address is one of these two countries, applicable taxes will be applied. If your shipping address is to the United States, we request your company?s Employer Identification Number (EIN) or Tax Identification Number (TIN). This is a unique 9-digit number assigned by the IRS and is required for all cross-border shipments. Failure to provide this number could result in delays to your order. If your shipping address is within the EU, but outside the Netherlands, then we are required to request your company's Value Added Tax (VAT, BTW, MwSt) number to be able to ship the goods tax-free. For all other countries, no taxes are levied on your orders. DON'T LIKE THESE PRICES? Tell us what you will pay for what order quantity. Shipping Charges for {product_name} All prices shown are ex-works KRAYDEN, but during the checkout process, you will be given several shipping options including Canada Post, TNT, UPS or the choice of using your own freight forwarder. Depending on your shipping address, the shipping charges will be calculated as follows:
Payment option for {product_name} During the checkout process, you will be presented with several payment options including:
Availability for {product_name} To the right of the product is a small icon that lets you know the availability and leadtime of the product. This leadtime is the time to ship the product and delivery times vary based on the method of delivery you select at the time you place your order. Contact us if anything is unclear or you need more assistance. |
{tab=Competitive Crossovers}
|
||||||||||||||||||||||||
{tab=Videos & Other Media}
|
Sorry, there are no related videos for {product_name} at this time. |
{tab=Product Reviews}
|
{review} |
{tab=View Blogs & Forum}
|
KRAYDEN is different. Unlike other business to business enterprises, we encourage our customers to discuss, critique, and otherwise comment on the products we offer. Get more technical information, read detailed posts, and see what customers have to say about about {product_name} on our Corporate Blog and Forum. |
{/tabs}