- 8-hour stencil life
- Printing up to <16mil pitch
- ROL1 & Bellcore GR-78 compliant
Product Description
Kester TSF-6502JCR is a no-clean tacky soldering flux formulated for high activity and robust performance. TSF-6502JCR enables excellent soldering on challenging surfaces, even under multiple thermal cycles, while leaving clear, aesthetically pleasing residues.
Product Key Features
- Stencil life: 8 hours (process dependent)
- Excellent printing characteristics to <16mil pitch
- Leaves bright/shiny solder joints after reflow
- Can reflow in air or nitrogen environments
- Classified as ROL1 per J-STD-004
- Compliant to Bellcore GR-78
Applications
- Nickel Surface Soldering
- OSP-Treated Copper Boards
- Multi-Reflow Processes
Packaging
Please select Package Type.
TDS, SDS & Technical Documents
Technical Specifications
Physical Properties
Viscosity
100000 mPa.s Viscosity is a measurement of a fluid’s resistance to flow.
Viscosity is commonly measured in centiPoise (cP). One cP is defined as
the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP.
A product like honey would have a much higher viscosity -around 10,000 cPs-
compared to water. As a result, honey would flow much slower out of a tipped glass than
water would.
The viscosity of a material can be decreased with an increase in temperature in
order to better suit an application