INSULCURE 11B
Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission

Main features
- Heat-Curing INSULCAST Epoxy Curing Agent
- 700 cP Application Viscosity
- 3-Hour 100 deg C Cure
Product Description
INSULCURE® 11B Epoxy Curing Agent is a rigid, temperature-resistant, heat-curing agent for compatible INSULCAST epoxy casting and encapsulation resins. The amber liquid is selected when extended pot life and elevated-temperature cured performance are required. Current supplier information lists a typical viscosity of 700 cP, a 300-minute pot life in the referenced system, and a three-hour cure schedule at 100°C. Final mix ratio and cured properties depend on the specific INSULCAST resin, so this component should be presented and processed only as part of a verified resin-hardener system.
Key features
- Heat-curing epoxy hardener: The curing agent is intended for compatible INSULCAST resin systems.
- Extended process window: Current supplier information lists a 300-minute pot life in the referenced system.
- Temperature-resistant rigid cure: The product is positioned for elevated-temperature epoxy systems.
Applications / Suitable for
- Curing compatible INSULCAST epoxy resins
- Heat-cured electrical potting systems
- Temperature-resistant epoxy casting systems
TDS, SDS & Technical Documents
Technical Specifications
No specifications available.
Additional Information
As-supplied / before-processing properties
Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Component role | Epoxy curing agent | N/A | As supplied |
| Appearance | Amber liquid | N/A | Product family description |
| Viscosity | 700 | cP | Current supplier product page |
| Pot life | 300 | min | Referenced system at 25°C |
| Reference cure | 3 | h | At 100°C |