Hysol GR360A-ST | Black Epoxy Mold Compound
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other


Main features
- Low cost of ownership
- 77% filler weight
- For Diodes, TO and DIP
Product Description
Hysol GR360A-ST epoxy molding compound delivers outstanding performance and ease of use. This "Green" environmentally friendly epoxy molding compound contains no bromine, antimony or phosphorus flame retardant. It provides the lowest cost of ownership with superior moldability and reliability.
Hysol GR360A-ST has an 77% filler loading and is typically used for Diodes, TO and DIP packages. It meets UL 94 V-0 Flammability at 6.35mm thickness. Its CTI, comparative tracking index value is 500V.
- GR360: CTI = 500 V (PLC-1 / IEC Material Group II)
- GR360A: CTI = 450 V (PLC-1 / IEC Material Group II)