Hysol GR180T | White Epoxy Mold Compound

Harmonization Code : 3907.30.00.15 | Epoxide resin, halogen-free

Hysol GR180T | White transmitting Epoxy Mold CompoundHysol GR180T | White Epoxy Mold Compound

Main features

  • Transmitting compound
  • High reliability
  • Good workability

Product Description

Hysol GR180T is a white, transmitting epoxy molding compound used for optical applications. This crystal silica filled (70%) product has been specifically designed to improve light transmittance and workability for optocouplers also knows as photo-couplers, optical isolators, or opto-isolators.

Hysol GR180T cures with heat and has been developed to be workable for transfer molding processes. It has been formulated to provide the best possible moldability for a wide range of molding process parameters.

Product Family

HYSOL GR180T

No longer available

This product is no longer available from Krayden. Please contact us so we can recommend an alternative product.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
White
Filler ContentFiller Content
70 %
Specific GravitySpecific Gravity
1.85
Chemical Properties
Moisture absorptionMoisture absorption
0.67 %
Physical Properties
Spiral Flow @ 175°CSpiral Flow @ 175°C
73 cm
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
195 °C
Curing Conditions
Transfer PressureTransfer Pressure
40 - 85 kg/cm2
Transfer TimeTransfer Time
5 - 12 s

Additional Information

Storage

Store product in the unopened container in a dry location. Storage information may be indicated on the product container labeling.

Optimal Storage: 5°C or below, in closed containers. After removal from cold storage, the material MUST be allowed to come to room temperature, in the sealed container, to avoid moisture contamination. The suggested waiting time for a standard 15 kg carton box is 24 hours.

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers