HARDMAN EPOWELD 58173

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

HARDMAN EPOWELD 58173

Main features

  • 5-Minute Gel Time
  • Cure Down to -18 deg C
  • Multi-Substrate Epoxy Bonding

Product Description

EPOWELD® 48173/58173 is an extra fast setting, two-component, room temperature curing epoxy adhesive designed to bond metal, wood, concrete, ceramics, and many plastics. It is highly effective for fast patching, fixturing, and repairs requiring quick handling strength, with the unique ability to cure at temperatures as low as -18°C (0°F).

Key features

  • Fast setting and gel time: Offers a quick 5-minute gel time and rapid handling strength for efficient repair and fixturing workflows.
  • Low temperature cure: Capable of curing at extreme temperatures as low as -18°C (0°F), allowing for versatile application environments.
  • Convenient mix ratio: Features a user-friendly 1:1 mix ratio by volume, simplifying dispensing and application.

Applications / Suitable for

  • Bonding metal, wood, concrete, ceramics, and many plastics.
  • Fast patching and fixturing applications.
  • General repairs requiring quick handling strength.
Product Family

HARDMAN EPOWELD 58173

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Mix RatioMix Ratio
1:1
Pot LifePot Life
5 minutes (Gel time) minutes

Additional Information

Technical properties

As-supplied / before-processing properties

Pre-cure physical and processing characteristics of mixed EPOWELD® 48173/58173.

Property Value Unit Method / condition
Appearance / Color (Mixed) Amber - -
Mix Ratio (Volume) 1:1 (100:100) - Part A to Part B
Mix Ratio (Weight) 100:94 - Part A to Part B
Viscosity (Mixed) 40,000 cps at 25°C
Specific Gravity (Mixed) 1.16 - at 25°C
Gel Time 5 minutes 4 gm mass at 25°C
Technical properties

After-processing / final-state properties

Typical cured mechanical properties of EPOWELD® 48173/58173 when tested at 25°C.

Property Value Unit Method / condition
Hardness 80 Shore D Tested at 25°C
Lap Shear Strength 3,000 psi Acid-etched Al/Al, cured 24 hrs @ 25°C, tested at 25°C
T-Peel Strength 1.8 pli Acid-etched Al/Al, cured 24 hrs @ 25°C, tested at 25°C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers