EPOCAST 169-1
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- Low-Density Epoxy Syntactic Resin
- Paste Consistency for Application
- Machinable Application Paste Material
Product Description
EPOCAST 169A-1 Resin is the resin component of a general-purpose, low-density epoxy syntactic material. It is supplied as a red-brown paste with a typical density of 0.56 g/cm³ at 25°C. The available resin-specific data emphasize its physical form, appearance, and low-density character for product identification and preparation before processing. This page covers EPOCAST 169A-1 Resin only; mixed-material processing information, qualification statements, storage data presented jointly for both components, and cured-system performance values have been excluded.
Key features
- Low-density resin: Typical as-supplied density of 0.56 g/cm³.
- Paste consistency: Supplied as a paste at 25°C.
- Red-brown appearance: Provides clear visual identification of the resin component.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied resin properties
Typical properties of the EPOCAST 169A-1 resin component before mixing or processing.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Red-brown | — | Visual; resin component |
| Density | 0.56 | g/cm³ | Typical value; ASTM D1622 |
| Viscosity / consistency | Paste | — | At 25°C; ASTM D2196 |