ELANTAS FR-1210

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

ELANTAS FR-1210

Main features

  • Low-Shrinkage Electrical Potting Resin
  • EA-02/EA-028/EA-87 Hardener Compatibility
  • 4,500 to 10,000 cP Mixed Viscosity

Product Description

CONAPOXY® FR-1210 Epoxy Encapsulant Resin is a tan, mineral-filled epoxy resin for two-component electrical potting and casting systems. The resin may be combined with CONACURE EA-02, EA-028, or EA-87 to produce systems with low shrinkage, controlled coefficient of thermal expansion, resistance to mechanical and thermal shock, and electrical insulation. The resin has a typical viscosity of 95,000 cP and specific gravity of 1.66 at 25°C. Published mixed-system viscosity ranges from 4,500 to 10,000 cP, with 24-hour room-temperature or two-hour 60°C cure schedules.

Key features

  • Mineral-filled epoxy resin: The resin is formulated for low-shrinkage potting and casting systems.
  • Three hardener options: EA-02, EA-028, and EA-87 provide different mixed viscosity and cured properties.
  • Room-temperature or heat cure: Published systems cure for 24 hours at 25°C or two hours at 60°C.

Applications / Suitable for

  • Electrical and electronic potting
  • Epoxy casting
  • Assemblies exposed to mechanical and thermal shock
Product Family

ELANTAS FR-1210

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Resin color Tan N/A As supplied
Resin specific gravity 1.66 N/A At 25°C
Resin viscosity 95,000 cP At 25°C
Mixed viscosity 4,500 to 10,000 cP Depending on hardener
Gel time 30 to 60 min At 25°C, hardener dependent
Room-temperature cure 24 h At 25°C
Alternate cure 2 h At 60°C
Shelf life 18 months At 20°C to 30°C in original containers
Technical properties

After-processing / final-state properties

Typical cured or final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Hardness 80 to 90 Shore D Depending on hardener
Tensile strength 6,500 to 8,050 psi Depending on hardener
Glass-transition temperature 70 to 90 °C Depending on hardener
Linear shrinkage 0.4 to 0.9 % Depending on hardener
Dielectric strength 375 V/mil All three documented systems
Volume resistivity 3.0 × 10¹³ to 4.2 × 10¹⁵ ohm·cm Depending on hardener

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers