ELANTAS EN-2553
Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

Main features
- Filled Flame-Retardant Polyurethane Potting System for Components
- 4,500 cP Mixed Viscosity
- UL 94 V-0 Classification
Product Description
CONATHANE® EN-2553 Polyurethane Encapsulant is a two-component, filled, flame-retardant polyurethane potting system for electronic components, modules, circuit boards, assemblies, and related devices. The brown Part A and black or blue Part B are mixed at 17:100 by weight to produce a typical initial viscosity of 4,500 cP and a 55-minute work life at 25°C. The system is documented for low-stress cure and thermal-shock resistance, with cure options of seven days at 25°C or 16 hours at 80°C. Typical cured properties include Shore A 95 hardness, 60% elongation, and UL 94 V-0 at 3 mm.
Key features
- Filled flame-retardant polyurethane: The cured material is documented as UL 94 V-0 at 3 mm.
- 55-minute work life: Typical initial mixed viscosity is 4,500 cP at 25°C.
- Low-stress protection: The system is documented for sensitive components and thermal-shock resistance.
Applications / Suitable for
- Electronic components and modules
- Circuit boards and assemblies
- Low-stress encapsulation of sensitive devices
TDS, SDS & Technical Documents
Technical Specifications
No specifications available.
Additional Information
As-supplied / before-processing properties
Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Part A viscosity | 300 | cP | At 25°C |
| Part B viscosity | 8,500 | cP | At 25°C |
| Part A specific gravity | 1.24 | N/A | At 25°C |
| Part B specific gravity | 1.49 | N/A | At 25°C |
| Mix ratio | 17:100 | parts by weight | Part A : Part B |
| Initial mixed viscosity | 4,500 | cP | At 25°C |
| Work life | 55 | min | At 25°C |
| Cure options | 7 days at 25°C; 16 h at 80°C | N/A | Documented schedules |
After-processing / final-state properties
Typical cured or final-state values under the stated system and test conditions. These values are not sales specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Hardness | 95 | Shore A | ASTM D2240 |
| Tensile strength | 1,050 | psi | ASTM D412 |
| Ultimate elongation | 60 | % | ASTM D412 |
| Tear strength | 140 | pli | ASTM D624 |
| Dielectric strength | 560 | V/mil | ASTM D149 |
| Volume resistivity | 3.1 × 10¹⁴ | ohm·cm | ASTM D257 at 25°C |
| Flammability classification | V-0 | UL 94 | At 3.0 mm |