DOWSIL Q2-1346
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg
Main features
- Low Sodium and Potassium Impurity Limits
- Clear Liquid Supplied Free from Suspended Matter
- Long 900-Day Shelf Life
Product Description
DOWSIL™ Q2-1346 Diluent is a silicone diluent supplied as a clear liquid for use in compatible silicone formulations. The product is manufactured to a controlled sales specification with requirements for appearance and low extractable sodium and potassium levels. It offers a long shelf life when stored in its original unopened container under the specified storage conditions.
Key Features
- Clear liquid free from suspended matter.
- Controlled maximum sodium content of 2.00 ppm (extracted water).
- Controlled maximum potassium content of 2.00 ppm.
- Long shelf life of 900 days in the original unopened container.
Suitable For
- Use in compatible DOWSIL™ silicone formulations.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Appearance
Clear Liquid Appearance at room temperature.
Additional Information
As-Supplied / Before-Processing Properties
| Property | Value |
|---|---|
| Appearance | Clear liquid, free from suspended matter |
| Sodium (in extracted water) | 2.00 ppm maximum |
| Potassium | 2.00 ppm maximum |
| Shelf Life | 900 days |
| Storage Conditions | No specific storage requirements; store in original unopened container |