DOWSIL 866 PRIMERLESS SILICONE ADHESIVE

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

DOWSIL 866 PRIMERLESS SILICONE ADHESIVE

Main features

  • Primerless Silicone Adhesion
  • Durable Silicone Formulation
  • EV/Automotive Component Assembly

Product Description

DOWSIL™ 866 Primerless Silicone Adhesive is a specialized silicone adhesive designed to provide robust bonding without the need for primer application. Suitable for evaluation in various industrial and automotive manufacturing contexts, including electric vehicle (EV) component assembly, this adhesive helps streamline production processes. Its reliable silicone chemistry ensures durable performance in demanding assembly and operational environments.

Key features

  • Primerless adhesion: Streamlines manufacturing processes by eliminating the need for separate primer preparation steps.
  • Durable silicone chemistry: Provides long-lasting reliability and environmental resistance for demanding applications.
  • EV component suitability: Supports advanced automotive assembly and electric vehicle manufacturing requirements.

Applications / Suitable for

  • Electric vehicle (EV) applications
  • Automotive component assembly
  • Industrial bonding operations
Product Family

DOWSIL 866

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Gray
Component SystemComponent System
1K
Specific GravitySpecific Gravity
1.29
Physical Properties
ViscosityViscosity
48,000 mPa.s
Mechanical Properties
ElongationElongation
210 %
Electrical Properties
Dielectric StrengthDielectric Strength
20 kV/mm
Volume ResistivityVolume Resistivity
2.00 E+15 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Color Gray - One-part
Viscosity 48,000 cP -
Heat Cure Time 60 minutes at 125°C
Heat Cure Time 30 minutes at 150°C
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Specific Gravity 1.29 - Cured
Durometer 57 Shore A -
Tensile Strength 925 psi -
Elongation 210 % -
Tear Strength 25 ppi Die B
Unprimed Adhesion - Lap Shear 774.5 psi To Aluminum
Dielectric Strength 500 volts/mil -
Volume Resistivity 2.00E+15 Ohm-cm -

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers