COOLTHERM 6732
Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others
Main features
- Hardener Component Thermal Interface Material
- 100:0.5 Controlled Mixing
- Thermally Conductive Thermal Interface
Product Description
Overview
CoolTherm® 6732 Hardener is the curing component of the CoolTherm® SC-6711 WHT/6732 Silicone Encapsulant system. It is supplied for use exclusively with CoolTherm® SC-6711 WHT Base at a 1:1 volume mix ratio to produce a thermally conductive silicone encapsulant for electronic potting and encapsulation applications. The hardener is not intended for standalone use.
Key Features
- Hardener component for the CoolTherm® SC-6711 WHT silicone encapsulant system.
- Designed for a 1:1 mix ratio by volume with SC-6711 WHT Base.
- Translucent liquid formulation.
- Used to produce a thermally conductive silicone encapsulant when mixed with the compatible base component.
Suitable For
- CoolTherm® SC-6711 WHT silicone encapsulant system
- Electronic potting and encapsulation (when mixed with SC-6711 WHT Base)
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Mix Ratio
100:0.5 The amount of a constituent divided by the total amount of all other constituents in a mixture
Additional Information
As-Supplied / Before-Processing Properties
| Component | Hardener (Part B) |
| Appearance | Translucent |
| Mix Ratio | 1:1 by volume with CoolTherm® SC-6711 WHT Base |