CONATHANE TU-801
Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

Main features
- Two-Component Polyurethane Part B Curative
- 100% Solids Flexible Casting System
- High-Toughness Chemical-Resistant Cured System
Product Description
CONATHANE® TU-801 Polyurethane Curative is the amber Part B curative used with compatible CONATHANE polyurethane resin systems, including TU-401. The paired two-component system is documented as a 100% solids polyurethane used for casting and potting flexible elastomers. System-level characteristics include toughness, high elongation, tensile and tear strength, ultraviolet stability, durability, and chemical resistance. ELANTAS lists a 100:51 resin-to-curative ratio for the TU-801 system, while final processing conditions and cured properties depend on the exact Part A pairing and must remain explicitly identified.
Key features
- Part B polyurethane curative: TU-801 is used with compatible CONATHANE resin components.
- 100% solids system: The paired polyurethane system is documented for casting and potting flexible elastomers.
- Tough elastomer profile: System descriptions cite high elongation, tensile strength, tear strength, and chemical resistance.
Applications / Suitable for
- Curative for compatible CONATHANE polyurethane systems
- Potting and casting flexible elastomers
- Industrial components requiring toughness and elongation
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Component role | Part B curative | N/A | As supplied |
| Color | Amber | N/A | As supplied |
| System chemistry | Polyurethane | N/A | Two-component system |
| System solids | 100 | % | Paired polyurethane system |
| Mix ratio with TU-401 | 100:51 | parts by weight | TU-401 resin : TU-801 curative |