CONAPOXY AD-10

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

CONAPOXY AD-10

Main features

  • One-Component Epoxy Adhesive/Potting Compound
  • 3,000 psi Aluminum Lap Shear
  • 93 to 204 deg C Cure Temperatures

Product Description

CONAPOXY® AD-10 Epoxy Adhesive is a one-component, 100% solids, non-flowing epoxy adhesive and miniature potting compound for electrical applications. The brown heat-cure paste is documented for bonding and sealing magnet and speaker assemblies, batteries, filters, structural materials, end-cap filling, staking, and miniature potting. It may be cured from 93°C to 204°C using the published time-temperature schedule and should not be applied above 3.2 mm thickness. Typical cured properties include Shore D 85 hardness, 3,000 psi aluminum lap shear strength, and dielectric strength above 375 V/mil.

Key features

  • One-component epoxy paste: The 100% solids material is supplied ready for heat-cure bonding, sealing, and miniature potting.
  • Wide heat-cure window: Published cure schedules range from 120 to 150 minutes at 93°C to two to four minutes at 204°C.
  • Electrical and structural properties: Typical cured data include 3,000 psi aluminum lap shear strength and dielectric strength above 375 V/mil.

Applications / Suitable for

  • Magnet and speaker assemblies
  • Batteries, filters, and end-cap filling
  • Miniature electronic potting, staking, and structural bonding
Product Family

CONAPOXY AD-10

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Product form One-component non-flow paste N/A As supplied
Chemistry Epoxy N/A 100% solids
Color Brown N/A As supplied
Specific gravity 1.27 N/A At 25°C
Flash point >94 °C ASTM D93
Shelf life 4 months At or below 25°C in original sealed containers
Minimum cure 120 to 150 min At 93°C
Maximum-speed cure 2 to 4 min At 204°C
Technical properties

After-processing / final-state properties

Typical cured or final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Hardness 85 Shore D ASTM D2240 at 25°C
Lap shear strength 3,000 psi ASTM D1002; aluminum-to-aluminum
Operating temperature -55 to 150 °C Documented range
Dielectric strength >375 V/mil ASTM D149
Dielectric constant 4.0 N/A ASTM D150 at 1 kHz and 25°C
Dissipation factor 0.006 N/A ASTM D150 at 1 kHz and 25°C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers