CLEANSAFE 787C
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

Main features
- Low-Foaming Lubrication Formulation
- Multi-Soil Cleaning Removal
- Ferrous and Non-Ferrous Alloys
Product Description
CleanSafe™ 787C Aqueous Cleaner is an ultra-low-foaming, alkaline aqueous cleaner for spray-in-air and agitated immersion cleaning equipment. It removes corrosion-inhibiting compounds, drawing and forming compounds, greases, hydraulic fluids, lubricants, oils, metalworking fluids, fingerprints, and particulates. The concentrated cleaner is suitable for ferrous and non-ferrous alloys, including untreated, alodined, and anodized aluminum; carbon steel; copper and copper alloys; stainless steel; titanium; and magnesium. Its non-foaming and non-scaling characteristics support controlled heated cleaning processes. :contentReference[oaicite:0]{index=0}
Key features
- Ultra-low-foaming performance: Formulated for spray-in-air and agitated immersion cleaning equipment.
- Broad soil removal: Removes corrosion-inhibiting compounds, metalworking fluids, greases, oils, hydraulic fluids, fingerprints, and particulates.
- Multi-metal compatibility: Suitable for documented ferrous and non-ferrous alloys, including aluminum, steel, copper alloys, titanium, and magnesium.
Applications / Suitable for
- Spray-in-air cleaning equipment
- Agitated immersion cleaning equipment
- Cleaning before non-destructive testing
- Removal of metalworking fluids and corrosion-inhibiting compounds
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied / before-processing properties
Typical physical and processing properties of CleanSafe™ 787C. Typical property data are not intended for specification purposes. :contentReference[oaicite:1]{index=1}
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Odor | Mild | — | Typical |
| Specific gravity | 1.08 | — | At 25 °C |
| pH value | 11.6 | — | At 10% concentration |
| Wash-bath concentration | 3–10 | % | Recommended process concentration |
| Wash-bath temperature | 140–160 (60–71) | °F (°C) | Recommended process range |
| DI-water rinse temperature | 140–160 (60–71) | °F (°C) | Recommended process range |
| Shelf life | 36 | months | Original sealed container above 50 °F (10 °C); protect from freezing |