BOSTIK LADH1531AC
Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.
Main features
- Sprayable neoprene contact adhesive
- Excellent green strength
- High water, oil & heat resistance
Product Description
Bostik LADH1531AC is a solvent-based neoprene contact adhesive designed for high-speed spray application in veneer bonding and other industrial laminating processes. The sprayable formulation delivers excellent green strength for immediate handling while providing high water, oil, and heat resistance after bonding. It is formulated for large-area, uniform adhesive coverage, enabling rapid processing and reduced production time in industrial manufacturing environments. :contentReference[oaicite:0]{index=0}
Key Features
- Sprayable neoprene contact adhesive for rapid, uniform adhesive application.
- Excellent green strength allows immediate handling after bonding.
- High water, oil, and heat resistance for demanding industrial applications.
- Designed for fast production with quick bond development for high-speed manufacturing.
Applications / Suitable For
- Veneer bonding
- Industrial laminating
- High-speed spray bonding
- Large-area contact bonding
- General industrial assembly
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Process Method
Solvent evaporation Product Type
Solvent-based neoprene contact adhesive Material category or functional product class.
Thermal Properties
Operating Temperature
Drying at 80°C °C Additional Information
Technical Properties
As-Supplied / Before-Processing Properties
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Product type | Neoprene solution contact adhesive | — | Sprayable solvent-based adhesive |
| Appearance | Tan liquid | — | Typical physical property |
| Total solids | 16 | % | Typical value |
| Viscosity | 185 | cP | LVF #2 @ 60 rpm, 25°C |
| Density | 6.7 | lb/gal | Typical value |
| Flash point (SCC) | -22 (-30) | °F (°C) | Typical value |
| Shelf life | 270 days (9 months) | — | Stored between 55–100°F (13–38°C) |
Technical Properties
After-Processing / Final-State Properties
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Dry adhesive coat weight | 2–5 | g/ft² | Applied to both substrates |
| Recommended drying condition | 80 | °C | 1–3 minutes in circulating air oven |
| Press pressure | 7 (0.5) | psi (kg/cm²) | 10–15 seconds for contact bonds |
| Green strength | Adequate for immediate handling | — | After recommended bonding process |
| Performance | High water, oil and heat resistance | — | Supplier description |