BONDERITE S-OT 310B
Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission
Main features
- PTFE Dry-Film Low-Friction Lubrication
- Oil, Solvent, and Chemical Resistance
- Metal and Rubber Coating Process
Product Description
BONDERITE® S-OT 310B ACHESON is a two-package resin-bonded dry film lubricant formulated as a PTFE dispersion in a solvent/water system. When combined with BONDERITE® L-GP T A COMP ACHESON, it forms a fluorocarbon coating in a thermosetting binder that delivers low-friction, stick-slip-free performance for metal and rubber substrates. The spray-applied coating provides durable lubrication and chemical resistance for industrial and consumer applications. :contentReference[oaicite:0]{index=0}
Key Features
- Two-package PTFE dry film lubricant for durable low-friction coatings.
- Produces stick-slip-free fluorocarbon coatings after curing.
- Suitable for metal and rubber substrates.
- Excellent resistance to oils, alcohols, ketones, dilute acids, esters, and aromatic hydrocarbons.
- One-component base mixed immediately before use with BONDERITE® L-GP T A COMP ACHESON.
Applications / Suitable for
- Metal components
- Rubber components
- Industrial mechanical assemblies
- Consumer product components
- Spray-applied dry film lubrication
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Product Type
wo-component PTFE coating Material category or functional product class.
Additional Information
Technical Properties
As-Supplied / Before-Processing Properties
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Technology | Lubricant | — | Supplier classification |
| Product type | PTFE dispersion in solvent/water | — | Supplier description |
| Application | Dry film lubricant | — | Supplier classification |
| Pigment | None | — | Wet product |
| Binder | Thermosetting resin | — | Wet product |
| Solids content | ~10.5 | % | Wet product |
| Color | Blue | — | Wet product |
| Flash point | 8 | °C | Wet product |
| Density | 910 | kg/m³ | Wet product |
| Theoretical coverage | 7.7 | m²/kg | @ 10 µm dry film thickness |
| Recommended storage temperature | 5–30 | °C | Unopened container |
| Shelf life | 18 | months | Unopened original packaging |
Technical Properties
After-Processing / Final-State Properties
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Coating color | Green | — | Cured coating |
| Coefficient of friction (static & kinetic) | ~0.06 | — | Cured coating |
| Recommended dry film thickness (metal) | 10–25 | µm | Typical application |
| Recommended dry film thickness (rubber) | 5–10 | µm | Typical application |
| Continuous service temperature | 150 | °C | Cured coating |
| Intermittent service temperature | 160 | °C | Cured coating |
| Chemical resistance | Resistant to oils, alcohols, ketones, chlorinated hydrocarbons, dilute acids, esters, aromatic hydrocarbons and gasohol | — | Cured coating |
| Curing schedule | 160°C / 60 min 180°C / 30 min 200°C / 10 min |
— | Substrate temperature |