BONDERITE S-FN 310A
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- PTFE Dry-Film Low-Friction Release
- Longer Wear Life than Pure PTFE
- 149 deg C Low-Temperature Cure
Product Description
BONDERITE S-FN 310 ACHESON (formerly EMRALON 310) is a two-component, phenolic resin-bonded PTFE dry film coating and lubricant. It cures at a low temperature of 300°F (149°C) and is designed to provide excellent surface adhesion, a low coefficient of friction, corrosion resistance, and good release properties on materials such as wood, metal, rubber, and plastics.
Key features
- Superior wear life: Delivers a longer wear life and more uniform thickness than pure PTFE coatings.
- Low friction and release: Provides an as-applied static friction coefficient between 0.05 and 0.07, along with excellent release properties.
- Low temperature cure: Enables application on substrates where conventional PTFE coatings cannot be used by curing at 300°F (149°C).
Applications / Suitable for
- Lubrication and release coating on wood, metal, rubber, and plastics.
- Applications requiring a low coefficient of friction.
- Substrates that require a low-temperature curing PTFE coating.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Product Type
Phenolic resin-bonded PTFE dry film coating and lubricant Material category or functional product class.
Thermal Properties
Operating Temperature
177°C (350°F) continuous service / 204°C (400°F) intermittent service °C Additional Information
Technical properties
As-supplied / before-processing properties
Physical and processing characteristics of mixed BONDERITE S-FN 310 ACHESON.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Mix Ratio (Weight) | 22:100 | - | Part A (White) to Part B (Blue) |
| Consistency | Liquid | - | - |
| Density (As Applied) | 8.2 | lb/gal | - |
| Flash Point | 46 (9) | °F (°C) | - |
| Pot Life | 24 | hours | - |
| Application Method | Spray | - | Cannot be dipped or brushed |
Technical properties
After-processing / final-state properties
Typical cured film properties of BONDERITE S-FN 310 ACHESON.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color (Cured) | Light green | - | Typical |
| Friction Coefficient (Static) | 0.05 to 0.07 | - | As applied |
| Service Temperature | 350 (177) | °F (°C) | - |
| Intermittent Temperature | 400 (204) | °F (°C) | Avoid temperatures in excess of this |