BONDERITE M-ED 1000
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- Nickel Acetate-Based Sealing Process
- Reduced Smut, Powdering, and Yellowing
- Commercial and Selected Military Anodizing Seal Processes
Product Description
BONDERITE® M-ED 1000 AERO is a liquid nickel acetate-based anodizing seal additive for clear, integral, and two-step electrolytically colored anodized aluminum. The sealing process improves corrosion resistance by penetrating and sealing the pores of the anodic film, while helping reduce smut, powdering, and yellowing commonly associated with anodizing seal operations. It is suitable for commercial and selected military sealing specifications.
Key Features
- Liquid nickel acetate sealing additive for anodized aluminum.
- Improves corrosion resistance by sealing anodic film pores.
- Helps reduce smut, powdering, and yellowing during anodizing seal operations.
- Suitable for clear, integral, and electrolytically colored anodized aluminum.
- Meets commercial and selected military sealing requirements.
Applications / Suitable for
- Clear anodized aluminum
- Integral colored anodized aluminum
- Two-step electrolytically colored anodized aluminum
- Anodizing seal baths
- Aerospace aluminum finishing
- Architectural and decorative anodizing
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Product Type
Electrodeposition pretreatment Material category or functional product class.
Additional Information
Technical Properties
As-Supplied / Before-Processing Properties
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Technology | Metal treatment | — | Supplier classification |
| Product Type | Anodizing additive | — | Supplier classification |
| Chemistry | Liquid nickel acetate-based seal process | — | Supplier description |
| Physical form | Liquid | — | Supplier description |
| Application | Anodized aluminum sealing | — | Supplier recommendation |
Technical Properties
After-Processing / Final-State Properties
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Working concentration | 1.5–2.5 | % by volume | 2.0% optimum |
| Operating temperature | 77–88 | °C | 85°C optimum |
| Sealing time | 5–15 | minutes | 10–12 minutes optimum |
| Operating pH | 5.7–6.0 | — | 5.8 optimum |
| Agitation | Mechanical agitation or recirculation | — | Recommended |