BONDERITE C-AK VITKL
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- Ferrous/Titanium Tenacious-Soil Removal
- Boeing BAC 5749 Compliance
- Low-Foaming Quick-Rinse Bath Control
Product Description
BONDERITE C-AK VITKL AERO (formerly TURCO VITRO-KLENE) is a brown granular, hot tank caustic cleaner formulated to remove drawing compounds, lube oil, rust preventive compounds, and other tenacious soils from ferrous and titanium alloys. It is designed to prepare surfaces for vitreous enameling and other processes requiring a high degree of cleanliness by producing a water-break-free surface.
Key features
- Aerospace qualified: Approved to Boeing BAC 5749 specifications.
- Optimized performance: Low foaming when used as recommended and readily rinses from parts with hot water.
- Safer profile: Nonflammable in concentrate or solution form, free of chromate, and low in chlorides.
Applications / Suitable for
- Hot tank cleaning of ferrous and titanium alloys.
- Pre-cleaning prior to vitreous enameling.
- Removing drawing compounds, lube oil, and rust preventive compounds.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Product Type
Alkaline cleaner Material category or functional product class.
Additional Information
Technical properties
As-supplied / before-processing properties
Physical characteristics and operating parameters for BONDERITE C-AK VITKL AERO[cite: 12].
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Brown granular mixture | - | - |
| Concentration Ratio | 60 to 75 | g/L | Added to cool agitated water |
| Operating Temperature | 70 to Boiling Point | °C | - |
| Flammability | Nonflammable | - | In concentrate or solution form |