BONDERITE C-AK MIL-ETCH
Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses
Main features
- Uniform Fine Satin or Frosted Etch
- Low-Foam Low-Mist Alkaline Etching
- BAC 5786 Operating Conditions
Product Description
BONDERITE® C-AK MIL-ETCH AERO is a granular alkaline cleaner and etchant formulated to produce a fine satin or frosted etch on aluminum and its alloys. The working solution develops a low-foam blanket to minimize caustic mist while providing excellent sequestering action that helps prevent scale and sludge buildup on tanks and heating coils. It is designed for aluminum surface preparation prior to deoxidizing, anodizing, and other finishing operations. :contentReference[oaicite:0]{index=0}
Key Features
- Produces a fine satin or frosted etch on aluminum and aluminum alloys.
- Low-foam alkaline formulation helps reduce caustic mist generation during processing.
- Excellent sequestering action minimizes scale and sludge buildup on tanks and heating coils.
- Suitable for aluminum pretreatment prior to deoxidizing and anodizing.
- Supports standard and BAC 5786 operating conditions.
Applications / Suitable for
- Aluminum surface etching
- Aluminum alloys
- Pretreatment before deoxidizing
- Pretreatment before anodizing
- Aerospace metal finishing
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Product Type
Granular alkaline cleaner and aluminum etchant Material category or functional product class.
Thermal Properties
Operating Temperature
37-72; 32 - 43 (for BAC 5786) °C Additional Information
Technical Properties
As-Supplied / Before-Processing Properties
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Technology | Alkaline cleaner / etchant | — | Supplier classification |
| Physical form | Granular powder | — | Supplier description |
| Application | Aluminum etching and cleaning | — | Supplier description |
| Bath make-up | 25–50 | lb per 100 gal | Initial bath preparation |
| Recommended storage | Cool, dry, ventilated area in sealed containers | — | Away from acidic materials |
| Shelf life | Not stated | — | Technical Process Bulletin |
Technical Properties
After-Processing / Final-State Properties
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Surface finish | Fine satin or frosted etch | — | On aluminum and its alloys |
| General operating concentration | 4–8 (30–60) | oz/gal (g/L) | General operation |
| General operating temperature | 37–72 | °C | 100–160°F |
| General treatment time | 5–10 | minutes | Optimum |
| BAC 5786 concentration | 3–5 (22.5–37.5) | oz/gal (g/L) | Approved as additive only |
| BAC 5786 temperature | 32–43 | °C | 90–110°F |
| BAC 5786 treatment time | 5–10 | minutes | Optimum |