BONDERITE C-AK 4215 NC-LT
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- Low-Temperature Multi-Metal Cleaning
- Fuel/Hydraulic Component Cleaning
- Chromate-Free Low-Foam Noncorrosive Formulation
Product Description
BONDERITE® C-AK 4215 NC-LT is a white granular alkaline cleaner developed for low-temperature cleaning of ferrous and nonferrous alloys using spray, immersion, and ultrasonic processes. The formulation is designed for cleaning fuel and hydraulic components and for preparing metal surfaces prior to metal bonding. Its balanced blend of organic surface-active agents provides controlled low-foam operation while remaining readily soluble, readily rinsable, free of chromates, and free of harsh caustics.
Key Features
- Low-temperature alkaline cleaner for spray, immersion, and ultrasonic cleaning.
- Suitable for ferrous and nonferrous alloys, including aluminum, steel, copper, and plated metals.
- Controlled low-foam formulation designed for severe agitation conditions.
- Readily soluble and free-rinsing for efficient cleaning and post-rinse performance.
- Chromate-free and free of harsh caustics.
Applications / Suitable for
- Fuel component cleaning
- Hydraulic component cleaning
- Cleaning prior to metal bonding
- Spray cleaning systems
- Immersion cleaning systems
- Ultrasonic cleaning systems
- Cleaning ferrous and nonferrous alloys
TDS, SDS & Technical Documents
Technical Specifications
Other Properties
Storage Temperature
−10 to 50°C °C General Properties
Appearance
White granular mix Appearance at room temperature.
Specific Gravity
Not Published Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume.
For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
Additional Information
Technical Properties
As-Supplied / Before-Processing Properties
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Technology | Metal Pretreatment | — | Supplier classification |
| Product Type | Alkaline Cleaner | — | Supplier classification |
| Application | Spray, Immersion, Ultrasonic | — | Supplier classification |
| Appearance | White granular mix | — | As supplied |
| Water solubility | Readily soluble | — | Supplier feature |
| Foam characteristics | Low foaming | — | Recommended concentrations and temperatures |
| Corrosion characteristics | Noncorrosive to aluminum, steel, copper and plated metals | — | Supplier feature |
| Chromate content | Chromate-free | — | Supplier feature |
| Storage temperature | -10 to 50 | °C | Recommended storage |
Technical Properties
After-Processing / Operating Properties
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Spray concentration | 7–15 | g/L | Spray cleaning |
| Spray operating temperature | 45–55 | °C | 2–4 minutes |
| Spray cleaning time | 2–4 | minutes | Supplier recommendation |
| Immersion concentration | 45–60 | g/L | Air or mechanical agitation recommended |
| Immersion operating temperature | 45–55 | °C | 5–10 minutes |
| Immersion cleaning time | 5–10 | minutes | Supplier recommendation |
| Ultrasonic concentration | 45–60 | g/L | Degas system before cleaning |
| Bath control | Total alkalinity titration to pH 4.0 | — | 1 N sulfuric acid with Bromcresol Green indicator |
| Bath maintenance | Maintain recommended concentration by adding fresh material | — | Supplier recommendation |
| Rinsing | Cold to warm water | — | Spray or overflowing immersion rinse |