BONDERITE C-AK 298
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- Non-Silicated Aluminum Immersion Cleaner
- Multi-Soil Removal and Free Rinsing
- 54 to 82 deg C Immersion Cleaning
Product Description
BONDERITE® C-AK 298 is a non-silicated alkaline immersion cleaner formulated for cleaning aluminum and aluminum alloys prior to anodizing and chemical conversion coating. The free-rinsing liquid formulation removes soils, oils, greases, inks, and wax-based markings while preparing aluminum surfaces for subsequent finishing operations. It is designed for high-temperature immersion cleaning in metal processing and fabrication applications. :contentReference[oaicite:0]{index=0}
Key Features
- Non-silicated alkaline cleaner formulated for aluminum and aluminum alloys.
- Free-rinsing immersion cleaner that prepares surfaces for anodizing and conversion coating.
- High-temperature operation for effective removal of oils, greases, inks, soils, and wax-based markings.
- Liquid concentrate designed for immersion cleaning processes.
Applications / Suitable for
- Cleaning aluminum and aluminum alloys
- Surface preparation before anodizing
- Surface preparation before chemical conversion coating
- High-temperature immersion cleaning
- Metal pretreatment operations
Technical Specifications
General Properties
Appearance
Brown liquid Appearance at room temperature.
Specific Gravity
Not Published Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume.
For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
Additional Information
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Technology | Industrial Cleaner | — | Supplier classification |
| Product type | Alkaline immersion cleaner | — | Supplier classification |
| Physical state | Liquid | — | As supplied |
| Color | Brown | — | As supplied |
| Chemistry | Non-silicated alkaline formulation | — | Supplier description |
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Application method | Immersion | — | Supplier recommendation |
| Working concentration | 8.2–18.6 | mL/L | Supplier operating range |
| Operating temperature | 54–82 (130–180) | °C (°F) | High-temperature immersion cleaning |
| Treatment time | 3–15 | minutes | Supplier operating range |
| Surface condition after cleaning | Free-rinsing, prepared for anodizing or conversion coating | — | Supplier application guidance |