Product Description
BONDERITE® C-AD 4215 AERO is a clear, colorless liquid additive formulated to enhance the cleaning performance of BONDERITE® C-AK 4215 AERO and other alkaline cleaners when difficult-to-remove soils are encountered. Suitable for both spray and immersion cleaning systems, the additive readily dissolves into alkaline cleaning baths, is compatible with ferrous and nonferrous alloys when used with a compatible base cleaner, and rinses cleanly from treated parts with cool to warm water.
Key Features
- Cleaning-performance enhancer for BONDERITE® C-AK 4215 AERO and other compatible alkaline cleaners.
- Low addition rate of only 1–2% by volume minimizes changes to existing cleaning processes.
- Suitable for spray and immersion systems with recommended air or mechanical agitation for immersion cleaning.
- Compatible with ferrous and nonferrous alloys when the selected alkaline cleaner is also compatible.
- Readily soluble and free-rinsing for efficient incorporation into alkaline cleaning baths.
Applications / Suitable for
- Enhancing alkaline cleaner performance
- Spray alkaline cleaning systems
- Immersion alkaline cleaning systems
- Cleaning difficult-to-remove soils
- Ferrous alloy cleaning processes
- Nonferrous alloy cleaning processes
TDS, SDS & Technical Documents
Technical Specifications
Other Properties
General Properties
Additional Information
As-Supplied / Before-Processing Properties
Supplier-published characteristics of BONDERITE® C-AD 4215 AERO.
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Technology | Metal Pretreatment | — | Supplier classification |
| Product Type | Additive | — | Supplier classification |
| Application | Immersion and Spray | — | Supplier classification |
| Appearance | Clear, colorless liquid | — | As supplied |
| Density | 0.951–0.961 | g/mL | Typical property |
| Flash Point | 110 | °C | Cleveland Open Cup Method |
| Storage Temperature | 0–40 | °C | Recommended storage |
| Shelf Life | 24 | months | Original unopened packaging |
After-Processing / Operating Properties
Supplier-recommended operating conditions when using BONDERITE® C-AD 4215 AERO with compatible alkaline cleaners.
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Recommended addition level | 1–2 | % by volume | Add after alkaline cleaner is fully mixed |
| Operating temperature | 60–80 | °C | Preferred operating range |
| Preferred operating temperature | 70 | °C | Supplier recommendation |
| Application methods | Spray and immersion | — | Compatible alkaline cleaning systems |
| Immersion agitation | Air or mechanical agitation recommended | — | Immersion cleaning |
| Rinsing | Cool to warm water rinse | — | Follow rinsing procedure of the selected alkaline cleaner |
| Compatibility | Ferrous and nonferrous alloys | — | Provided the base cleaner is compatible with the substrate |