Product Description
AXAREL™ 3000 Solvent Cleaner is a high-performance precision cleaning solvent formulated for removing oils, greases, waxes, silicones, buffing compounds, lapping compounds, adhesives, resins, and other manufacturing contaminants from metal and electronic components. The solvent is designed for vapor degreasing and immersion cleaning processes, providing excellent cleaning performance with fast drying and low residue characteristics for industrial cleaning applications.
Key Features
- High solvency cleaner for removing a broad range of industrial contaminants.
- Fast-drying formulation that leaves low surface residue after cleaning.
- Compatible with precision cleaning processes, including vapor degreasing and immersion cleaning.
Applications / Suitable for
- Precision cleaning of metal components
- Electronic component cleaning
- Vapor degreasing operations
- Immersion cleaning systems
- Removal of oils, greases, waxes, silicones, adhesives, resins, and machining contaminants
TDS, SDS & Technical Documents
Technical Specifications
Thermal Properties
Flash Point
96 °C The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor.
Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
General Properties
Specific Gravity
0.83 Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume.
For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
Vapor Pressure
0.18 mmHg Physical Properties
Viscosity
2.2 mPa.s Viscosity is a measurement of a fluid’s resistance to flow.
Viscosity is commonly measured in centiPoise (cP). One cP is defined as
the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP.
A product like honey would have a much higher viscosity -around 10,000 cPs-
compared to water. As a result, honey would flow much slower out of a tipped glass than
water would.
The viscosity of a material can be decreased with an increase in temperature in
order to better suit an application
Additional Information
Technical Properties
As-Supplied / Before-Processing Properties
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Appearance | Clear liquid | — | As supplied |
| Specific Gravity (25°C) | 1.45 | — | 25°C |
| Viscosity (25°C) | 0.61 | cP | 25°C |
| Boiling Point | 54 | °C | Published property |
| Flash Point | None | — | Published property |
| Kauri-Butanol (KB) Value | 128 | — | Published property |