LOCTITE ABLESTIK QMI519

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite Ablestik QMI519

Main features

  • Void free bondline
  • Hydrophobic
  • Strongest Die attach

Product Description

LOCTITE ABLESTIK QMI519 silver filled conductive adhesive is a proprietary Hybrid BMI/Acrylate resin, recommended for use in bonding integrated circuits and components to metal leadframes. It is is designed to achieve UPHs several orders of magnitude higher than conventional oven cured adhesives. After 1500 hours of testing it is, by far, the strongest die attach paste (almost double of 8302 which comes at the 2nd place). The initial adhesion is in "mid-range" but it increases heavily during aging.

LOCTITE ABLESTIK QMI519 maximum productivity is realized through in-line cure, either on the die bonder using a post diebond heater or on the wirebonder preheater. Studies have also shown improved coplanarity in parts cured on the die bonder. This product and its use may be covered by patent 5,717,034 and by one or more pending patent applications.

LOCTITE ABLESTIK QMI519 is an electrically and thermally conductive, hydrophobic product that achieves void free bondlines and stability at high temperatures. It is typically used for SOIC, SOP, QFP and QFN type packages and on a wide variety of metals and ceramic surfaces, Copper, Silver, Palladium and Alloy 42. It is a great product of choice for PPF leadframes.

 

SkipCure Process

  • ≥10 seconds @ 200°C

Typical Cure

  • 15minutes @ 185°C
  • 15minutes @ 200 to 220°C
Product Family

ABLESTIK QMI519

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 28 days
CA Shipping in 12 weeks
EU Shipping in 25 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific GravitySpecific Gravity
3.8
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
75 °C
Thermal ConductivityThermal Conductivity
3.8 W/m.K
Physical Properties
Thixotropic indexThixotropic index
4.2
ViscosityViscosity
9,000 mPa.s

Additional Information

QMI519 has excellent adhesion when it comes to bare die on PPF leadframes
 
 
 

QMI 519 - Die shear strength @ 260°C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers