ABLESTIK GA 47-2LV

Harmonization Code : 5906100000 | Adhesive tape of a width not exceeding 20cm

ABLESTIK GA 47-2LV

Main features

  • Gyro-Flotation-Fluid-Compatible Instrument Bonding
  • 25 ppm/deg C Linear Thermal Expansion
  • 2-Hour 95 deg C Cure

Product Description

LOCTITE® ABLESTIK GA 47-2LV is a green, low-viscosity, heat-cured epoxy instrument adhesive. It is documented as compatible with conventional gyro flotation fluids and has a coefficient of thermal expansion that approximates aluminum within a normal temperature range. The material provides a typical viscosity of 50,000 mPa·s, a 30-minute work life at 25°C, and guideline cure options of 2 hours at 95°C or 4 hours at 75°C. Cured aluminum-to-aluminum lap shear strength is reported as 13.8 N/mm². :contentReference[oaicite:0]{index=0}

Key features

  • Gyro-fluid compatibility: Documented compatibility with conventional gyro flotation fluids supports evaluation for applicable instrument assemblies. :contentReference[oaicite:1]{index=1}
  • Aluminum-matched thermal expansion: The coefficient of thermal expansion approximates that of aluminum within a normal temperature range. :contentReference[oaicite:2]{index=2}
  • Heat-cure flexibility: Guideline cure schedules include 2 hours at 95°C or 4 hours at 75°C. :contentReference[oaicite:3]{index=3}

Applications / Suitable for

  • Instrument bonding applications
  • Assemblies involving conventional gyro flotation fluids
  • Bonding aluminum components under the documented cure conditions
Product Family

ABLESTIK GA 47-2LV

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Green
Chemistry TypeChemistry Type
Epoxy
Specific GravitySpecific Gravity
2.1
Work life @25°CWork life @25°C
0.5 hours
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
95 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties and processing characteristics of the adhesive before cure. :contentReference[oaicite:4]{index=4}

Property Value Unit Method / condition
Technology Epoxy As supplied
Appearance Green liquid or paste TDS appearance and SDS physical state
Viscosity 50,000 mPa·s (cP) Test method and temperature not stated
Specific gravity 2.1 As supplied
Work life 30 minutes At 25°C
Shelf life 365 days At -40°C
Cure schedule 2 hours or 4 hours 2 hours at 95°C or 4 hours at 75°C; guideline recommendations
Technical properties

After-processing / final-state properties

Typical properties and performance data for the cured adhesive. Values are reference data rather than product specifications. :contentReference[oaicite:5]{index=5}

Property Value Unit Method / condition
Hardness 90 Shore D Test method and cure condition not stated
Glass-transition temperature 95.0 °C Method and cure condition not stated
Coefficient of linear thermal expansion — below Tg 25 ppm/°C Below Tg; method and cure condition not stated
Lap shear strength — aluminum to aluminum 13.8 (2,000) N/mm² (psi) Substrate preparation, bondline, cure condition, test method, and test temperature not stated

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers